公开(公告)号:US20140069613A1
公开(公告)日:2014-03-13
申请号:US13965897
申请日:2013-08-13
Applicant: Industrial Technology Research Institute
Inventor: Chia-Ming LIU , Lien-Tai CHEN , Tsing-Tang SONG , Chin-Tien YANG , Szu-Ju LI
IPC: F28F1/10
Abstract: A cooling apparatus is disclosed. The cooling apparatus includes a carrier and a flat-plate type cooling conduit. The flat-plate type cooling conduit is made of a high thermal conductive material and disposed on or in the carrier. The flat-plate type cooling conduit includes a conduit portion and a flat plate portion. The conduit portion has a conducting hole for conducting a coolant, and the flat plate portion is adhered to the carrier for allowing the coolant to perform heat exchange through a large contact area between the flat plate portion and the carrier. In addition, a cooling source gel can be used to perform heat exchange with the coolant in the conducting hole in order to improve the heat exchange efficiency of the cooling apparatus, and to effectively reduce the temperature of the carrier.
Abstract translation: 公开了一种冷却装置。 冷却装置包括载体和平板型冷却导管。 平板式冷却导管由高导热材料制成并设置在载体上或载体上。 平板式冷却导管包括导管部分和平板部分。 导管部具有用于导引冷却剂的导电孔,并且平板部分粘附到载体上,以允许冷却剂通过平板部分和载体之间的大的接触面进行热交换。 此外,为了提高冷却装置的热交换效率,可以使用冷却源凝胶与导电孔内的冷却剂进行热交换,有效降低载体的温度。
-
公开(公告)号:US20130152737A1
公开(公告)日:2013-06-20
申请号:US13707931
申请日:2012-12-07
Applicant: Industrial Technology Research Institute
Inventor: Lien-Tai CHEN , Ruoh-Huey UAN , Tsing-Tang SONG , Zhi-Long CHEN , Chun-Chen CHIANG , Ya-Hui LIN
IPC: B22F9/18
CPC classification number: B22F9/18 , B22F1/0025 , B22F9/24 , B22F2301/255 , B82Y40/00
Abstract: Disclosed is a method for preparing silver nanowire. The method includes: providing a first solution and a second solution; mixing the first solution and the second solution to obtain a third solution including a plurality of silver nanowires; and performing a purification procedure on the third solution to obtain the silver nanowires. Particularly, the first solution includes a capping agent dispersed in a first alcohol solvent, and the second solution includes a silver salt and a metal precursor dispersed in a second alcohol solvent, wherein the metal precursor has a formula: MXn or MXn.m(H2O) wherein M is Cu2+, Sn4+, or Ni2+, X is Cl−, Br−, I−, SCN−, SO42−, NO3−, or C2O42−, n is 1-4, m is 1-6, and M has a valence equal to the absolute value of the product of n and a valence of X.
Abstract translation: 公开了一种制备银纳米线的方法。 该方法包括:提供第一溶液和第二溶液; 混合第一溶液和第二溶液以获得包含多个银纳米线的第三溶液; 并在第三溶液上进行纯化程序以获得银纳米线。 特别地,第一溶液包括分散在第一醇溶剂中的封端剂,第二溶液包括分散在第二醇溶剂中的银盐和金属前体,其中金属前体具有下式:MXn或MXn.m(H 2 O )其中M为Cu2 +,Sn4 +或Ni2 +,X为Cl-,Br-,I-,SCN-,SO42-,NO3-或C2O42-,n为1-4,m为1-6,M为 的价数等于n的乘积和X的化合价的绝对值。
-