公开(公告)号:US20230055650A1
公开(公告)日:2023-02-23
申请号:US17787397
申请日:2020-11-24
Applicant: JFE Steel Corporation
Inventor: Mitsuhiro Okatsu , Masao Yuga , Toshiharu Hirama
IPC: C21D9/08 , F16L9/02 , C22C38/54 , C22C38/50 , C22C38/48 , C22C38/46 , C22C38/44 , C22C38/42 , C22C38/06 , C22C38/04 , C22C38/02 , C22C38/00 , C21D8/10 , C21D6/00
Abstract: Provided herein is a high-strength seamless steel pipe, and a method for manufacturing same. A high-strength seamless steel pipe of the present invention has a yield strength of 758 MPa or more, and a KILIMIT value of 23.0 MPa√m or more as an evaluation index of sulfide stress corrosion cracking resistance.
-
公开(公告)号:US12227816B2
公开(公告)日:2025-02-18
申请号:US17787397
申请日:2020-11-24
Applicant: JFE Steel Corporation
Inventor: Mitsuhiro Okatsu , Masao Yuga , Toshiharu Hirama
IPC: C21D9/08 , C21D6/00 , C21D8/10 , C22C38/00 , C22C38/02 , C22C38/04 , C22C38/06 , C22C38/42 , C22C38/44 , C22C38/46 , C22C38/48 , C22C38/50 , C22C38/54 , F16L9/02
Abstract: Provided herein is a high-strength seamless steel pipe, and a method for manufacturing same. A high-strength seamless steel pipe of the present invention has a yield strength of 758 MPa or more, and a KILIMIT value of 23.0 MPa√m or more as an evaluation index of sulfide stress corrosion cracking resistance.
-
公开(公告)号:US20230023397A1
公开(公告)日:2023-01-26
申请号:US17787402
申请日:2020-11-24
Applicant: JFE Steel Corporation
Inventor: Mitsuhiro Okatsu , Masao Yuga , Toshiharu Hirama
IPC: C21D9/08 , C22C38/00 , C22C38/02 , C22C38/04 , C22C38/06 , C22C38/16 , C22C38/22 , C22C38/24 , C22C38/26 , C22C38/32 , C21D8/10
Abstract: Provided herein is a high-strength seamless steel pipe, and a method for manufacturing same. A high-strength seamless steel pipe of the present invention has a steel microstructure with a prior austenite grain size of 11.0 or more in terms of a grain size number in compliance with ASTM E112, and has a yield strength of 862 MPa or more and 965 MPa or less.
-
-