Separation of purified potassium sulfate from glaserite
    1.
    发明授权
    Separation of purified potassium sulfate from glaserite 有权
    从闪锌矿中分离纯化的硫酸钾

    公开(公告)号:US07604792B2

    公开(公告)日:2009-10-20

    申请号:US12252591

    申请日:2008-10-16

    IPC分类号: C01D5/00 B03B5/60

    CPC分类号: C01D5/00

    摘要: A method can, in one general aspect, include steps for the recovery of potassium sulfate and mirabilite from glaserite. In another general aspect, a method includes dissolving glaserite in water at an elevated temperature to produce a saturated or nearly saturated solution, and cooling the solution to a temperature where potassium sulfate and mirabilite will crystallize from the solution as stable phases. In yet another general aspect, a method includes adding glaserite to a saturated solution of glaserite in water and mixing for enough time at a temperature where the glaserite will decompose into potassium sulfate and mirabilite as stable phases. In yet another general aspect, a method includes separating potassium sulfate from mirabilite using a froth floatation process.

    摘要翻译: 在一个一般方面,一种方法可以包括从闪锌矿中回收硫酸钾和芒硝的步骤。 在另一个总体方面,一种方法包括在高温下将芒桃石溶解在水中以产生饱和或接近饱和的溶液,并将溶液冷却至硫酸钾和芒硝从溶液中以稳定相结晶的温度。 在另一个总体方面,一种方法包括将镁硅酸盐在水溶液中加入氟硅藻土的饱和溶液,并在闪锌矿分解成硫酸钾和芒硝作为稳定相的温度下混合足够的时间。 在另一个总体方面,一种方法包括使用泡沫漂浮法从芒硝中分离出硫酸钾。

    Separation of Purified Potassium Sulfate from Glaserite
    2.
    发明申请
    Separation of Purified Potassium Sulfate from Glaserite 有权
    从硅酸盐分离纯化的硫酸钾

    公开(公告)号:US20090104106A1

    公开(公告)日:2009-04-23

    申请号:US12252591

    申请日:2008-10-16

    IPC分类号: C01D5/00

    CPC分类号: C01D5/00

    摘要: A method can, in one general aspect, include steps for the recovery of potassium sulfate and mirabilite from glaserite. In another general aspect, a method includes dissolving glaserite in water at an elevated temperature to produce a saturated or nearly saturated solution, and cooling the solution to a temperature where potassium sulfate and mirabilite will crystallize from the solution as stable phases. In yet another general aspect, a method includes adding glaserite to a saturated solution of glaserite in water and mixing for enough time at a temperature where the glaserite will decompose into potassium sulfate and mirabilite as stable phases. In yet another general aspect, a method includes separating potassium sulfate from mirabilite using a froth floatation process.

    摘要翻译: 在一个一般方面,一种方法可以包括从闪锌矿中回收硫酸钾和芒硝的步骤。 在另一个总体方面,一种方法包括在高温下将芒桃石溶解在水中以产生饱和或接近饱和的溶液,并将溶液冷却至硫酸钾和芒硝从溶液中以稳定相结晶的温度。 在另一个总体方面,一种方法包括将镁硅酸盐在水溶液中加入氟硅藻土的饱和溶液,并在闪锌矿分解成硫酸钾和芒硝作为稳定相的温度下混合足够的时间。 在另一个总体方面,一种方法包括使用泡沫漂浮法从芒硝中分离出硫酸钾。