公开(公告)号:US20090213317A1
公开(公告)日:2009-08-27
申请号:US12078596
申请日:2008-04-02
申请人: Jia-Hau Jian , Chih-Ho Chiu , Cheng-Jung Chiang , Chung-Ching Hsieh , Te-Sheng Chen , Norio Sugiura
发明人: Jia-Hau Jian , Chih-Ho Chiu , Cheng-Jung Chiang , Chung-Ching Hsieh , Te-Sheng Chen , Norio Sugiura
IPC分类号: G02F1/1341 , G02F1/1339
CPC分类号: G02F1/1341 , G02F1/1339 , G02F2001/13415
摘要: A method for manufacturing a liquid crystal display panel is provided. The method includes: providing a first substrate and a second substrate; providing a plurality of liquid crystal drops on the first substrate, wherein two adjacent liquid crystal drops in X direction is kept by a distance d1 mm, and two adjacent liquid crystal drops in Y direction is kept by a distance d2 mm, each liquid crystal drop is G mg, d1≦16.7, d2≦15.4, and G≦1; and connecting the first substrate and the second substrate so that the liquid crystal drops are sealed between the first substrate and the second substrate.
摘要翻译: 提供一种液晶显示面板的制造方法。 该方法包括:提供第一基板和第二基板; 在第一基板上设置多个液晶滴,其中X方向上的两个相邻的液晶滴保持距离d1mm,并且在Y方向上的两个相邻的液晶滴保持距离d2mm,每个液晶滴 是G mg,d1 <= 16.7,d2 <= 15.4,G <= 1; 以及连接所述第一基板和所述第二基板,使得所述液晶滴被密封在所述第一基板和所述第二基板之间。
-
公开(公告)号:US08049863B2
公开(公告)日:2011-11-01
申请号:US12878493
申请日:2010-09-09
申请人: Jia-Hau Jian , Chih-Ho Chiu , Cheng-Jung Chiang , Chung-Ching Hsieh , Te-Sheng Chen , Norio Sugiura
发明人: Jia-Hau Jian , Chih-Ho Chiu , Cheng-Jung Chiang , Chung-Ching Hsieh , Te-Sheng Chen , Norio Sugiura
IPC分类号: G02F1/1341 , G02F1/1337 , G02F1/13
CPC分类号: G02F1/1341 , G02F1/1339 , G02F2001/13415
摘要: A method for manufacturing a liquid crystal display panel is provided. The method includes: providing a first substrate and a second substrate; providing a plurality of liquid crystal drops on the first substrate, wherein two adjacent liquid crystal drops in X direction is kept by a distance d1 mm, and two adjacent liquid crystal drops in Y direction is kept by a distance d2 mm, each liquid crystal drop is G mg, d1 16.7, d2 15.4, and G 1; connecting the first substrate and the second substrate so that the liquid crystal drops are sealed between the first substrate and the second substrate; and polymerizing the polymeric components of the liquid crystal drops while applying a predetermined voltage to the liquid crystal drops.
摘要翻译: 提供一种液晶显示面板的制造方法。 该方法包括:提供第一基板和第二基板; 在第一基板上设置多个液晶滴,其中X方向上的两个相邻的液晶滴保持距离d1mm,并且在Y方向上的两个相邻的液晶滴保持距离d2mm,每个液晶滴 是G mg,d1 16.7,d2 15.4和G 1; 连接第一基板和第二基板,使得液晶滴被密封在第一基板和第二基板之间; 并且在对液晶滴施加预定电压的同时聚合液晶的聚合物组分。
-
公开(公告)号:US20110032470A1
公开(公告)日:2011-02-10
申请号:US12878493
申请日:2010-09-09
申请人: Jia-Hau Jian , Chih-Ho Chiu , Cheng-Jung Chiang , Chung-Ching Hsieh , Te-Sheng Chen , Norio Sugiura
发明人: Jia-Hau Jian , Chih-Ho Chiu , Cheng-Jung Chiang , Chung-Ching Hsieh , Te-Sheng Chen , Norio Sugiura
IPC分类号: G02F1/1341
CPC分类号: G02F1/1341 , G02F1/1339 , G02F2001/13415
摘要: A method for manufacturing a liquid crystal display panel is provided. The method includes: providing a first substrate and a second substrate; providing a plurality of liquid crystal drops on the first substrate, wherein two adjacent liquid crystal drops in X direction is kept by a distance d1 mm, and two adjacent liquid crystal drops in Y direction is kept by a distance d2 mm, each liquid crystal drop is G mg, d1 16.7, d2 15.4, and G 1; connecting the first substrate and the second substrate so that the liquid crystal drops are sealed between the first substrate and the second substrate; and polymerizing the polymeric components of the liquid crystal drops while applying a predetermined voltage to the liquid crystal drops.
摘要翻译: 提供一种液晶显示面板的制造方法。 该方法包括:提供第一基板和第二基板; 在第一基板上设置多个液晶滴,其中X方向上的两个相邻的液晶滴保持距离d1mm,并且在Y方向上的两个相邻的液晶滴保持距离d2mm,每个液晶滴 是G mg,d1 16.7,d2 15.4和G 1; 连接第一基板和第二基板,使得液晶滴被密封在第一基板和第二基板之间; 并且在对液晶滴施加预定电压的同时聚合液晶的聚合物组分。
-
公开(公告)号:US08349413B2
公开(公告)日:2013-01-08
申请号:US12368281
申请日:2009-02-09
申请人: Cheng-Jung Chiang , Chih-Ho Chiu , Chung-Ching Hsieh , Chia-Hsuan Pai , Bo-Hsin Huang , Te-Sheng Chen
发明人: Cheng-Jung Chiang , Chih-Ho Chiu , Chung-Ching Hsieh , Chia-Hsuan Pai , Bo-Hsin Huang , Te-Sheng Chen
IPC分类号: C09K19/00
CPC分类号: G02F1/1337 , G02F1/133711 , G02F1/133788 , G02F2001/133715 , G02F2001/133742 , G02F2001/133765 , G02F2001/13415 , G02F2201/40
摘要: A liquid crystal display panel including a first substrate, a second substrate, a liquid crystal layer, and a polymer stabilized alignment layer is provided. The second substrate is disposed opposite to the first substrate. The liquid crystal layer is disposed between the first substrate and the second substrate. The polymer stabilized alignment layer is disposed between the first substrate and the liquid crystal layer, and an average surface roughness of the polymer stabilized alignment layer is greater than or equal to 10 nm.
摘要翻译: 提供了包括第一基板,第二基板,液晶层和聚合物稳定取向层的液晶显示面板。 第二基板与第一基板相对设置。 液晶层设置在第一基板和第二基板之间。 聚合物稳定化取向层设置在第一基板和液晶层之间,聚合物稳定取向膜的平均表面粗糙度大于或等于10nm。
-
公开(公告)号:US20100015363A1
公开(公告)日:2010-01-21
申请号:US12368281
申请日:2009-02-09
申请人: Cheng-Jung Chiang , Chih-Ho Chiu , Chung-Ching Hsieh , Chia-Hsuan Pai , Bo-Hsin Huang , Te-Sheng Chen
发明人: Cheng-Jung Chiang , Chih-Ho Chiu , Chung-Ching Hsieh , Chia-Hsuan Pai , Bo-Hsin Huang , Te-Sheng Chen
IPC分类号: G02F1/1337
CPC分类号: G02F1/1337 , G02F1/133711 , G02F1/133788 , G02F2001/133715 , G02F2001/133742 , G02F2001/133765 , G02F2001/13415 , G02F2201/40
摘要: A liquid crystal display panel including a first substrate, a second substrate, a liquid crystal layer, and a polymer stabilized alignment layer is provided. The second substrate is disposed opposite to the first substrate. The liquid crystal layer is disposed between the first substrate and the second substrate. The polymer stabilized alignment layer is disposed between the first substrate and the liquid crystal layer, and an average surface roughness of the polymer stabilized alignment layer is greater than or equal to 10 nm.
摘要翻译: 提供了包括第一基板,第二基板,液晶层和聚合物稳定取向层的液晶显示面板。 第二基板与第一基板相对设置。 液晶层设置在第一基板和第二基板之间。 聚合物稳定化取向层设置在第一基板和液晶层之间,聚合物稳定取向膜的平均表面粗糙度大于或等于10nm。
-
公开(公告)号:US20070049753A1
公开(公告)日:2007-03-01
申请号:US11269320
申请日:2005-11-07
申请人: Kuen-Yuan Hwang , An-Bang Duh , Chih-Fu Chen , Cheng-Jung Chiang
发明人: Kuen-Yuan Hwang , An-Bang Duh , Chih-Fu Chen , Cheng-Jung Chiang
IPC分类号: C07D251/54
CPC分类号: C07D251/56
摘要: The present invention relates to a method for preparing amino phosphate flame retardants. Melamine and phosphoric acid substances are used as a starting material, AND then the starting material reacts in the absence of solvents at a temperature ranging from 40 to 200° C. to obtain powdery amino phosphate compounds used as flame retardants. Since the reaction free of solvents is carried out under a condition of lower temperature, the powdery amino phosphate compounds can be obtained without drying steps. Therefore, not only the contaminations caused by solvent volatilization can be avoided, but also the process of preparing the product is simplified and the cost of the product is reduced.
摘要翻译: 本发明涉及一种制备氨基磷酸酯阻燃剂的方法。 使用三聚氰胺和磷酸物质作为原料,然后起始物质在不存在溶剂的情况下在40〜200℃的温度下反应,得到用作阻燃剂的粉末状氨基磷酸酯化合物。 由于没有溶剂的反应在较低温度的条件下进行,所以可以在没有干燥步骤的情况下获得粉状氨基磷酸酯化合物。 因此,不仅可以避免由溶剂挥发引起的污染,而且简化了产品的制备过程,降低了产品的成本。
-
公开(公告)号:US07507819B2
公开(公告)日:2009-03-24
申请号:US11269320
申请日:2005-11-07
申请人: Kuen-Yuan Hwang , An-Bang Duh , Chih-Fu Chen , Cheng-Jung Chiang
发明人: Kuen-Yuan Hwang , An-Bang Duh , Chih-Fu Chen , Cheng-Jung Chiang
IPC分类号: C07D251/54
CPC分类号: C07D251/56
摘要: The present invention relates to a method for preparing amino phosphate flame retardants. Melamine and phosphoric acid substances are used as a starting material, AND then the starting material reacts in the absence of solvents at a temperature ranging from 40 to 200° C. to obtain powdery amino phosphate compounds used as flame retardants. Since the reaction free of solvents is carried out under a condition of lower temperature, the powdery amino phosphate compounds can be obtained without drying steps. Therefore, not only the contaminations caused by solvent volatilization can be avoided, but also the process of preparing the product is simplified and the cost of the product is reduced.
摘要翻译: 本发明涉及一种制备氨基磷酸酯阻燃剂的方法。 使用三聚氰胺和磷酸物质作为原料,然后起始物质在不存在溶剂的情况下在40〜200℃的温度下反应,得到用作阻燃剂的粉末状氨基磷酸酯化合物。 由于没有溶剂的反应在较低温度的条件下进行,所以可以在没有干燥步骤的情况下获得粉状氨基磷酸酯化合物。 因此,不仅可以避免由溶剂挥发引起的污染,而且简化了产品的制备过程,降低了产品的成本。
-
-
-
-
-
-