1.
公开(公告)号:US07713502B2
公开(公告)日:2010-05-11
申请号:US11574199
申请日:2005-08-31
申请人: Joachim Koehler , Ralf Zuber , Matthias Binder , Volker Baenisch , Marco Lopez
发明人: Joachim Koehler , Ralf Zuber , Matthias Binder , Volker Baenisch , Marco Lopez
IPC分类号: C22B11/00
CPC分类号: H01M8/008 , B01D11/0203 , C08J11/08 , C08J2327/12 , C22B7/009 , C22B11/046 , C22B11/048 , H01M2008/1095 , Y02P10/214 , Y02P20/544 , Y02P20/582 , Y02W30/701 , Y02W30/86
摘要: The invention relates to a process for recycling fuel cell components containing fluorine-containing and precious metal-containing constituents: in this process, the fluorine-containing constituents are separated off from the precious metal-containing constituents by treatment with a medium present in the supercritical state. Preference is given to using water as supercritical medium. After the fluorine-containing constituents have been separated off, the precious metal-containing residues can be recovered in a recycling process without harmful fluorine or hydrogen fluoride emissions. The fluorine-containing constituents can likewise be recovered. The process is used in the recovery of precious metals and/or fluorine-containing constituents from membrane fuel cells, electrolysis cells, batteries, sensors and other electrochemical devices.
摘要翻译: 本发明涉及一种用于再循环含有含氟和含贵金属的成分的燃料电池组件的方法:在该方法中,通过用存在于超临界中的介质处理从含贵金属的成分中分离出含氟成分 州。 优先使用水作为超临界介质。 含氟成分被分离后,含有贵金属的残留物可以在循环过程中回收,而不会有有害的氟或氟化氢排放。 含氟成分同样可以回收。 该方法用于从膜燃料电池,电解槽,电池,传感器和其它电化学装置回收贵金属和/或含氟成分。
-
2.
公开(公告)号:US20080064771A1
公开(公告)日:2008-03-13
申请号:US11574199
申请日:2005-08-31
申请人: Joachim Koehler , Ralf Zuber , Matthias Binder , Volker Baenisch , Marco Lopez
发明人: Joachim Koehler , Ralf Zuber , Matthias Binder , Volker Baenisch , Marco Lopez
CPC分类号: H01M8/008 , B01D11/0203 , C08J11/08 , C08J2327/12 , C22B7/009 , C22B11/046 , C22B11/048 , H01M2008/1095 , Y02P10/214 , Y02P20/544 , Y02P20/582 , Y02W30/701 , Y02W30/86
摘要: The invention relates to a process for recycling fuel cell components containing fluorine-containing and precious metal-containing constituents: in this process, the fluorine-containing constituents are separated off from the precious metal-containing constituents by treatment with a medium present in the supercritical state. Preference is given to using water as supercritical medium. After the fluorine-containing constituents have been separated off, the precious metal-containing residues can be recovered in a recycling process without harmful fluorine or hydrogen fluoride emissions. The fluorine-containing constituents can likewise be recovered. The process is used in the recovery of precious metals and/or fluorine-containing constituents from membrane fuel cells, electrolysis cells, batteries, sensors and other electrochemical devices.
摘要翻译: 本发明涉及一种用于再循环含有含氟和含贵金属成分的燃料电池组件的方法:在该方法中,通过用存在于超临界中的介质处理含氟成分与贵金属成分分离 州。 优先使用水作为超临界介质。 含氟成分被分离后,含有贵金属的残留物可以在循环过程中回收,而不会有有害的氟或氟化氢排放。 含氟成分同样可以回收。 该方法用于从膜燃料电池,电解槽,电池,传感器和其它电化学装置回收贵金属和/或含氟成分。
-