Polymer emulsion coatings for cellulosic substrates with improved barrier properties
    1.
    发明授权
    Polymer emulsion coatings for cellulosic substrates with improved barrier properties 有权
    具有改进的阻隔性能的纤维素基材的聚合物乳液涂料

    公开(公告)号:US07427444B2

    公开(公告)日:2008-09-23

    申请号:US10620654

    申请日:2003-07-16

    IPC分类号: B32B23/04

    摘要: A cellulosic product such as paper coating composition is disclosed comprising aqueous-based semi-crystalline vinyl acetate-ethylene polymer emulsions, containing crystalline ethylene segments, which are useful for imparting oil, grease, solvent, water, and moisture vapor resistance. The polymer emulsions are prepared via the direct aqueous-based free radical emulsion polymerization of ethylene with various other comonomers. The semi-crystalline aqueous-based polymer emulsions of this invention have a crystalline melting point and a crystalline heat of fusion ranging from 5 to 100 J/g. The semi-crystalline aqueous-based emulsion polymers of this invention can be used directly as a paper or paperboard coating for imparting oil, grease, solvent, water, and moisture vapor resistance. Further, the present invention provides a repulpable paper and paperboard.

    摘要翻译: 公开了一种纤维素产品,例如纸涂料组合物,其包含含有结晶乙烯链段的水性半结晶乙酸乙烯酯 - 乙烯聚合物乳液,其可用于赋予油,油脂,溶剂,水和耐湿蒸气性。 通过乙烯与各种其它共聚单体的直接水基自由基乳液聚合制备聚合物乳液。 本发明的半结晶水性聚合物乳液具有5至100J / g的结晶熔点和熔融结晶热。 本发明的半结晶水性乳液聚合物可以直接用作赋予油,油脂,溶剂,水和耐湿蒸气性的纸或纸板涂料。 此外,本发明提供了一种可再造纸和纸板。

    Test for measuring adhesion of polymer binders to a heated metal surface
    2.
    发明授权
    Test for measuring adhesion of polymer binders to a heated metal surface 失效
    测试聚合物粘合剂与加热的金属表面的粘合力

    公开(公告)号:US06918305B2

    公开(公告)日:2005-07-19

    申请号:US10024967

    申请日:2001-12-19

    IPC分类号: G01N19/04 G01N3/08

    CPC分类号: G01N19/04

    摘要: The following method is used to measure the adhesion of a polymer binder to a heated metal surface:A metal plate is attached to a heated (350° F.; 177° C.) platform and allowed to equilibrate to the temperature of the platform. A polymer emulsion binder is applied to a substrate, such as cotton fabric, and an end of the coated substrate is attached to a tensile measuring apparatus. The coated side of the coated substrate is pressed onto the heated metal plate; e.g., using a 3-lb lab roller. After a length of time to cause drying and/or partial cure of the binder (approximately 30 seconds), the metal plate and the tensile measuring device are separated at a given uniform speed. The amount of force needed to remove the substrate from the metal plate is recorded.

    摘要翻译: 使用以下方法测量聚合物粘合剂对加热的金属表面的粘附性:将金属板连接到加热的(350°F; 177℃)平台上,并使其平衡至平台的温度。 将聚合物乳液粘合剂施加到诸如棉织物的基底上,并且将涂覆的基底的一端连接到拉伸测量装置。 将涂覆的基材的涂布面压在加热的金属板上; 例如使用3磅实验辊。 经过一段时间使粘合剂干燥和/或部分固化(约30秒)后,金属板和拉伸测量装置以给定的均匀速度分离。 记录从金属板除去基板所需的力的量。