Method for electroslag remelting of a manganese-copper-nickel alloy
    1.
    发明授权
    Method for electroslag remelting of a manganese-copper-nickel alloy 失效
    锰铜镍合金电渣重熔方法

    公开(公告)号:US4161399A

    公开(公告)日:1979-07-17

    申请号:US904165

    申请日:1978-05-08

    IPC分类号: B22D23/10 C22B4/06 C22B9/18

    CPC分类号: C22B4/06 B22D23/10 C22B9/18

    摘要: A manganese-copper-nickel alloy is remelted to form high quality ingots or slabs which are capable of undergoing hot-working in the "as cast" form by electroslag remelting the alloy under a flux composition prepared by fusing a mixture consisting essentially of from about 50% to about 85% barium fluoride and from about 15% to about 50% calcium fluoride, by weight.

    摘要翻译: 将锰 - 铜 - 镍合金重熔以形成能够以“铸造”形式进行热加工的高质量铸锭或板坯,通过电渣法将合金重熔在通过将基本上由约 50%至约85%的氟化钡和约15%至约50%的氟化钙。

    Method for electroslag remelting of a copper-nickel alloy
    2.
    发明授权
    Method for electroslag remelting of a copper-nickel alloy 失效
    铜镍合金电渣重熔方法

    公开(公告)号:US4161398A

    公开(公告)日:1979-07-17

    申请号:US904166

    申请日:1978-05-08

    IPC分类号: B22D23/10 C22B4/06 C22B9/18

    CPC分类号: C22B9/18 B22D23/10 C22B4/06

    摘要: A copper-nickel alloy is remelted to form high quality ingots or slabs which are capable of undergoing hot-working in the "as cast" form by electroslag remelting the alloy under a flux composition prepared by fusing a mixture consisting essentially of from about 35% to about 75% barium fluoride and from about 25% to about 65% calcium fluoride, by weight.

    摘要翻译: 铜镍合金被重熔以形成能够以“铸造”形式进行热加工的高质量铸锭或板坯,其中电渣通过将基本上由约35% 至约75%的氟化钡和约25%至约65%的氟化钙。

    Refining nickel base superalloys
    3.
    发明授权
    Refining nickel base superalloys 失效
    精炼镍基超级合金

    公开(公告)号:US4049470A

    公开(公告)日:1977-09-20

    申请号:US681297

    申请日:1976-04-29

    申请人: Claudia J. Burton

    发明人: Claudia J. Burton

    IPC分类号: C22C1/02 C22F1/10

    CPC分类号: C22C1/023

    摘要: A process for producing a low iron nickel base superalloy having a very low selenium content. The process includes the steps of: preparing a superalloy melt containing, by weight, at least 60% nickel, no more than 1% iron, and more than 0.0004% selenium; maintaining the melt in contact with a calcium and/or magnesium bearing substance for a period of time sufficient to allow for reaction between selenium and calcium and/or magnesium, and a lowering of said melt's selenium content to a level below 0.0003%, said selenium removal being carried out in a substantially oxygen free atmosphere; casting the melt; and heat treating the cast metal.

    摘要翻译: 一种生产硒含量非常低的低铁镍基超级合金的方法。 该方法包括以下步骤:制备含有至少60%镍,不超过1%铁和0.0004%以上硒的超合金熔体; 使熔融物与含钙和/或镁的物质接触足以允许硒和钙和/或镁之间的反应的时间以及所述熔体的硒含量降低到0.0003%以下的水平,所述硒 去除在基本上无氧的气氛中进行; 铸造熔体; 并对铸造金属进行热处理。