公开(公告)号:US07341974B2
公开(公告)日:2008-03-11
申请号:US10486403
申请日:2003-01-03
申请人: Jung Hwa Kang , Won Ho Lee , Min Ho Kil , Hyun Jong Shin , Byung Yul Choi , Yeon Shick Yoo , Young Hyun Choe , Ju Yeon Park
发明人: Jung Hwa Kang , Won Ho Lee , Min Ho Kil , Hyun Jong Shin , Byung Yul Choi , Yeon Shick Yoo , Young Hyun Choe , Ju Yeon Park
IPC分类号: B01J23/00
CPC分类号: B01J23/002 , B01J23/8876 , B01J37/0236 , B01J2523/00 , C07C51/252 , C07C57/04 , B01J2523/13 , B01J2523/54 , B01J2523/68 , B01J2523/842 , B01J2523/845
摘要: The present invention relates to a method for preparing a catalyst for partial oxidation of propylene, particularly a method for preparing a catalyst for preparing an acrylic acid, using an organic acid such as a citric acid, maleic acid and oxalic acid. The complex oxide catalyst according to the invention, when used in the gas phase catalytic oxidation of propylene, may produce acrolein in high yield.
摘要翻译: 本发明涉及一种制备用于丙烯部分氧化的催化剂的方法,特别是使用有机酸如柠檬酸,马来酸和草酸制备丙烯酸的催化剂的方法。 当用于丙烯的气相催化氧化时,根据本发明的复合氧化物催化剂可以高产率生产丙烯醛。
-
公开(公告)号:US07491673B2
公开(公告)日:2009-02-17
申请号:US10498901
申请日:2003-07-11
申请人: Jung Hwa Kang , Won Ho Lee , Min Ho Kil , Hyun Jong Shin , Byung Yul Choi , Yeon Shick Yoo , Young Hyun Choi , Ju Yeon Park
发明人: Jung Hwa Kang , Won Ho Lee , Min Ho Kil , Hyun Jong Shin , Byung Yul Choi , Yeon Shick Yoo , Young Hyun Choi , Ju Yeon Park
IPC分类号: B01J23/02 , B01J23/22 , B01J23/26 , B01J23/28 , B01J23/30 , B01J23/31 , B01J23/847 , B01J23/86 , B01J23/88 , B01J23/881 , B01J23/885 , B01J23/888 , B01J37/03
CPC分类号: B01J37/0232 , B01J23/002 , B01J23/8885 , B01J37/0221 , B01J37/03 , B01J2523/00 , C07C51/252 , C07C57/04 , B01J2523/17 , B01J2523/24 , B01J2523/55 , B01J2523/68 , B01J2523/69
摘要: The present invention provides a method for producing a catalyst comprising an inert carrier an a mixed metal oxide as a catalytically active component supported on the inert carrier, the method comprising the steps of: a) adding organic acid(s) into solvent(s) and salt of each metal component which will form a mixed metal oxide, to prepare a catalyst precursor solution for the mixed metal oxide; b) adjusting pH of the catalyst precursor solution using a basic solution; c) containing the catalyst precursor solution for the mixed metal oxide, of which the pH is adjusted, on the inert carrier, d) removing the solvent(s); and e) calcining the resultant from step d. The catalyst produced by the present method has improved reproducibility, activity and yield, while maintaining a high selectivity.
摘要翻译: 本发明提供了一种制备催化剂的方法,所述催化剂包含惰性载体和负载在惰性载体上的作为催化活性组分的混合金属氧化物,所述方法包括以下步骤:a)将有机酸加入到溶剂中, 和将形成混合金属氧化物的各种金属组分的盐,以制备用于混合金属氧化物的催化剂前体溶液; b)使用碱性溶液调节催化剂前体溶液的pH; c)在惰性载体上含有其中调节pH的混合金属氧化物的催化剂前体溶液,d)除去溶剂; 和e)煅烧步骤d的结果。 通过本方法制备的催化剂在保持高选择性的同时提高了再现性,活性和产率。
-