摘要: This document describes a process/strategy for age hardening nickel based alloys to create desirable properties with reduced energy expenditure. The inventive process introduces isolated atom nucleation sites to accelerate the nucleation rate by approximately 36 times, thereby permitting age hardening to occur in significantly less time and with significantly less energy expenditure.
摘要翻译: 本文件描述了一种用于时效硬化镍基合金以降低能量消耗产生理想特性的方法/策略。 本发明的方法引入了分离的原子成核位点以将成核速率加速约36倍,从而允许在显着更少的时间和显着更少的能量消耗下发生时效硬化。
-
公开(公告)号:US20140352853A1
公开(公告)日:2014-12-04
申请号:US13903501
申请日:2013-05-28
申请人: Ke Han , Pingli Mao , Yan Xin
发明人: Ke Han , Pingli Mao , Yan Xin
IPC分类号: C22F1/10
CPC分类号: C22F1/10 , C22C19/057
摘要: This document describes a process/strategy for age hardening nickel based alloys to create desirable properties with reduced energy expenditure. The inventive process introduces isolated atom nucleation sites to accelerate the nucleation rate by approximately 36 times, thereby permitting age hardening to occur in significantly less time and with significantly less energy expenditure.
摘要翻译: 本文件描述了一种用于时效硬化镍基合金以降低能量消耗产生理想特性的方法/策略。 本发明的方法引入了分离的原子成核位点以将成核速率加速约36倍,从而允许在显着更少的时间和显着更少的能量消耗下发生时效硬化。
-
公开(公告)号:US20120012234A1
公开(公告)日:2012-01-19
申请号:US12838004
申请日:2010-07-16
申请人: Ke Han , Pingli Mao , Yan Xin
发明人: Ke Han , Pingli Mao , Yan Xin
CPC分类号: C22C19/057 , C22F1/10
摘要: This document describes a process/strategy for age hardening nickel based alloys to create desirable properties with reduced energy expenditure. The inventive process introduces isolated atom nucleation sites to accelerate the nucleation rate by approximately 36 times, thereby permitting age hardening to occur in significantly less time and with significantly less energy expenditure.
摘要翻译: 本文件描述了一种用于时效硬化镍基合金以降低能量消耗产生理想特性的方法/策略。 本发明的方法引入了分离的原子成核位点以将成核速率加速约36倍,从而允许在显着更少的时间和显着更少的能量消耗下发生时效硬化。
-
公开(公告)号:US20170029926A1
公开(公告)日:2017-02-02
申请号:US15291157
申请日:2016-10-12
申请人: Ke Han , Pingli Mao , Yan Xin
发明人: Ke Han , Pingli Mao , Yan Xin
CPC分类号: C22F1/10 , C22C19/057
摘要: This document describes a process/strategy for age hardening nickel based alloys to create desirable properties with reduced energy expenditure. The inventive process introduces isolated atom nucleation sites to accelerate the nucleation rate by approximately 36 times, thereby permitting age hardening to occur in significantly less time and with significantly less energy expenditure.
摘要翻译: 本文件描述了一种用于时效硬化镍基合金以降低能量消耗产生理想特性的方法/策略。 本发明的方法引入了分离的原子成核位点以将成核速率加速约36倍,从而允许在显着更少的时间和显着更少的能量消耗下发生时效硬化。
-
-
-