Low iron high transmission glass with boron oxide for improved optics, durability and refining, and corresponding method
    1.
    发明授权
    Low iron high transmission glass with boron oxide for improved optics, durability and refining, and corresponding method 有权
    具有氧化硼的低铁高透光性玻璃,用于改善光学,耐久性和精炼以及相应的方法

    公开(公告)号:US08298972B2

    公开(公告)日:2012-10-30

    申请号:US13067997

    申请日:2011-07-14

    IPC分类号: C03C6/02 C03C3/087

    摘要: This invention relates to a high transmission low iron glass that includes boron oxide. The boron oxide, added to this low iron glass, has the effect of improving glass refining, homogeneity and quality (lower seed count) through its flux action and improves glass optical parameters of green and clear glass through the change in refractive index and surface tension. Boron oxide lends to broader and weaker absorption band of such transition element(s) as iron which additionally improves the transmittance of low iron clear glass in certain example embodiments of this invention. In certain example embodiments, the addition of boron oxide in certain quantities in advantageous in that it improves the chemical durability of the glass by decreasing the USPX (or USPXIII) value of the glass via suppression of the silica, sodium ions in the glass structure.

    摘要翻译: 本发明涉及包含氧化硼的高透光低铁玻璃。 添加到该低铁玻璃中的氧化硼通过其助焊剂作用具有改善玻璃精炼,均匀性和质量(较低种子计数)的效果,并通过折射率和表面张力的变化改善绿色和透明玻璃的玻璃光学参数 。 硼氧化物适合于铁的这种过渡元素的更宽和更弱的吸收带,其在本发明的某些示例性实施方案中另外提高了低铁透明玻璃的透射率。 在某些示例性实施方案中,加入一定量的氧化硼是有利的,因为通过玻璃结构中的二氧化硅钠离子的降低来降低玻璃的USPX(或USPXIII)值,从而提高了玻璃的化学耐久性。

    Low iron high transmission glass with boron oxide for improved optics, durability and refining, and corresponding method
    2.
    发明申请
    Low iron high transmission glass with boron oxide for improved optics, durability and refining, and corresponding method 有权
    具有氧化硼的低铁高透光性玻璃,用于改善光学,耐久性和精炼以及相应的方法

    公开(公告)号:US20110275506A1

    公开(公告)日:2011-11-10

    申请号:US13067997

    申请日:2011-07-14

    IPC分类号: C03C6/04

    摘要: This invention relates to a high transmission low iron glass that includes boron oxide. The boron oxide, added to this low iron glass, has the effect of improving glass refining, homogeneity and quality (lower seed count) through its flux action and improves glass optical parameters of green and clear glass through the change in refractive index and surface tension. Boron oxide lends to broader and weaker absorption band of such transition element(s) as iron which additionally improves the transmittance of low iron clear glass in certain example embodiments of this invention. In certain example embodiments, the addition of boron oxide in certain quantities in advantageous in that it improves the chemical durability of the glass by decreasing the USPX (or USPXIII) value of the glass via suppression of the silica, sodium ions in the glass structure.

    摘要翻译: 本发明涉及包含氧化硼的高透光低铁玻璃。 添加到该低铁玻璃中的氧化硼通过其助焊剂作用具有改善玻璃精炼,均匀性和质量(较低种子计数)的效果,并通过折射率和表面张力的变化改善绿色和透明玻璃的玻璃光学参数 。 硼氧化物适合于铁的这种过渡元素的更宽和更弱的吸收带,其在本发明的某些示例性实施方案中另外提高了低铁透明玻璃的透射率。 在某些示例性实施方案中,加入一定量的氧化硼是有利的,因为通过玻璃结构中的二氧化硅钠离子的降低来降低玻璃的USPX(或USPXIII)值,从而提高了玻璃的化学耐久性。

    Low iron high transmission glass with boron oxide for improved optics, durability and refining, and corresponding method
    3.
    发明申请
    Low iron high transmission glass with boron oxide for improved optics, durability and refining, and corresponding method 审中-公开
    具有氧化硼的低铁高透光性玻璃,用于改善光学,耐久性和精炼以及相应的方法

    公开(公告)号:US20100255980A1

    公开(公告)日:2010-10-07

    申请号:US12385318

    申请日:2009-04-03

    IPC分类号: C03C3/089 C03C3/095

    摘要: This invention relates to a high transmission low iron glass that includes boron oxide. The boron oxide, added to this low iron glass, has the effect of improving glass refining, homogeneity and quality (lower seed count) through its flux action and improves glass optical parameters of green and clear glass through the change in refractive index and surface tension. Boron oxide lends to broader and weaker absorption band of such transition element(s) as iron which additionally improves the transmittance of low iron clear glass in certain example embodiments of this invention. In certain example embodiments, the addition of boron oxide in certain quantities in advantageous in that it improves the chemical durability of the glass by decreasing the USPX (or USPXIII) value of the glass via suppression of the silica, sodium ions in the glass structure.

    摘要翻译: 本发明涉及包含氧化硼的高透光低铁玻璃。 添加到该低铁玻璃中的氧化硼通过其助焊剂作用具有改善玻璃精炼,均匀性和质量(较低种子计数)的效果,并通过折射率和表面张力的变化改善绿色和透明玻璃的玻璃光学参数 。 硼氧化物适合于铁的这种过渡元素的更宽和更弱的吸收带,其在本发明的某些示例性实施方案中另外提高了低铁透明玻璃的透射率。 在某些示例性实施方案中,加入一定量的氧化硼是有利的,因为通过玻璃结构中的二氧化硅钠离子的降低来降低玻璃的USPX(或USPXIII)值,从而提高了玻璃的化学耐久性。