公开(公告)号:US20230000076A1
公开(公告)日:2023-01-05
申请号:US17781667
申请日:2021-02-09
发明人: Aiqin Wang , Aiping Hui , Fangfang Yang , Yuru Kang , Bin Mu , Qin Wang , Yongfeng Zhu
IPC分类号: A01N25/12 , A23K20/28 , A23K40/30 , A23K40/10 , A23K20/105 , A23K20/163 , A23K20/111 , A23K20/121 , A01P1/00 , A01N35/02 , A01N43/08
摘要: Disclosed is a method for preparing an attapulgite-based pH-responsive antibacterial material, including: directly spraying a natural aldehyde-based antibacterial agent onto an attapulgite powder under stirring, and constantly stirring the attapulgite powder for 20-30 min; grinding the attapulgite powder in a ball mill for 30-60 min to obtain a ground attapulgite powder; placing the ground attapulgite powder in a stirred tank, and spraying a chitosan-citric acid aqueous solution onto the ground attapulgite powder; after spraying, constantly stirring the ground attapulgite powder for 30-120 min; and finally drying the ground attapulgite powder to obtain a dried attapulgite powder, sieving the dried attapulgite powder to obtain a sieved attapulgite powder, and packaging the sieved attapulgite powder to obtain the antibacterial material.
-
2.
公开(公告)号:US11999856B2
公开(公告)日:2024-06-04
申请号:US17269803
申请日:2019-07-12
发明人: Bin Mu , Aiqin Wang , Xiaowen Wang , Aiping Hui , Yuru Kang , Wenbo Wang , Li Zong , Yongfeng Zhu , Qin Wang
CPC分类号: C09C1/0006 , C09C3/006 , C09C3/041 , C09C3/043 , C01P2006/37 , C01P2006/62 , C01P2006/63 , C01P2006/64
摘要: The present disclosure relates to a method for preparation of a high temperature-resistant bismuth yellow pigment. The method comprises: mixing an oxide which served as a matrix and dopan with a bismuth source, a vanadium source, or a molybdenum source, and then placing the mixture into a mill for grinding to obtain a precursor; further calcining and crushing the precursor to obtain the high temperature-resistant bismuth yellow pigment powder. The bismuth yellow pigment has a bright color, a b* value greater than 90, a stable performance, and a high heat-resistance above 800° C. The method is environmentally friendly without waste, and reaction conditions are simple. Doping of BiVO4 crystal lattices by incorporation of oxides can be achieved, so that the particle size and distribution of the bismuth yellow pigment can be effectively controlled while the color performance of the bismuth yellow pigment is greatly improved.
-
公开(公告)号:US11700849B2
公开(公告)日:2023-07-18
申请号:US17781667
申请日:2021-02-09
发明人: Aiqin Wang , Aiping Hui , Fangfang Yang , Yuru Kang , Bin Mu , Qin Wang , Yongfeng Zhu
IPC分类号: A01N25/12 , A23K20/28 , A23K20/163 , A23K40/10 , A23K40/30 , A23K20/105 , A23K20/111 , A23K20/121 , A01P1/00 , A01N35/02 , A01N43/08
CPC分类号: A01N25/12 , A01N35/02 , A01N43/08 , A01P1/00 , A23K20/105 , A23K20/111 , A23K20/121 , A23K20/163 , A23K20/28 , A23K40/10 , A23K40/30
摘要: Disclosed is a method for preparing an attapulgite-based pH-responsive antibacterial material, including: directly spraying a natural aldehyde-based antibacterial agent onto an attapulgite powder under stirring, and constantly stirring the attapulgite powder for 20-30 min; grinding the attapulgite powder in a ball mill for 30-60 min to obtain a ground attapulgite powder; placing the ground attapulgite powder in a stirred tank, and spraying a chitosan-citric acid aqueous solution onto the ground attapulgite powder; after spraying, constantly stirring the ground attapulgite powder for 30-120 min; and finally drying the ground attapulgite powder to obtain a dried attapulgite powder, sieving the dried attapulgite powder to obtain a sieved attapulgite powder, and packaging the sieved attapulgite powder to obtain the antibacterial material.
-
-