    摘要: A composite material is disclosed along with the method of making the same. The material comprises a tough grade of cemented carbide granule dispersed with a hard brittle grade of cemented carbide granules to form a matrix. The quantity of hard, brittle cemented carbide granules is between 20% to 60% of the total composition. Such material functions to improve wear resistance without sacrificing toughness.

    Composite cemented carbide
    2.
    发明授权
    Composite cemented carbide 失效
    复合硬质合金

    公开(公告)号:US5593474A

    公开(公告)日:1997-01-14

    申请号:US228099

    申请日:1988-08-04

    IPC分类号: B22F1/00 C22C1/05 C22C29/08

    CPC分类号: C22C1/051 B22F1/0003

    摘要: A composite material is disclosed along with the method of making the same. The material comprises a tough grade of cemented carbide granule dispersed with a hard brittle grade of cemented carbide granules to form a matrix. The quantity of hard, brittle cemented carbide granules is between 20% to 60% of the total composition. Such material functions to improve wear resistance without sacrificing toughness.

    摘要翻译: 公开了一种复合材料及其制造方法。 该材料包括坚硬级别的硬质合金颗粒,其分散有硬脆的级别的硬质合金颗粒以形成基体。 硬质脆性硬质合金颗粒的数量在总组合物的20%至60%之间。 这种材料的功能是改善耐磨性而不牺牲韧性。

    Hard facing
    3.
    发明授权
    Hard facing 失效
    硬面

    公开(公告)号:US5051112A

    公开(公告)日:1991-09-24

    申请号:US501421

    申请日:1990-03-28

    IPC分类号: B23K35/32 B23K35/40 E21B10/50

    摘要: A hard facing rod is made by mixing particles of tungsten carbide, particles of a metal binder, and a temporary organic binder. The mixture is pressed, preferably by extrusion, into the form of a rod. The organic binder is removed and the rod is heated to a sufficient temperature to sinter the metal particles together without melting so that the rod has a residual porosity in the range of from 5 to 20%. Such a rod is used for hard facing a metal surface in lieu of conventional tube-rods. The technique permits a high proportion of tungsten carbide relative to the metal matrix and provides uniform distribution of carbide particles in the hard facing.

    摘要翻译: 通过混合碳化钨颗粒,金属粘合剂颗粒和临时有机粘合剂来制备硬面棒。 将混合物优选通过挤出压制成棒的形式。 去除有机粘合剂并将棒加热到足够的温度以将金属颗粒烧结在一起而不熔化,使得棒的残留孔隙率在5至20%的范围内。 这种棒用于硬面对金属表面以代替常规管棒。 该技术允许相对于金属基体的高比例的碳化钨,并且在硬质面中提供均匀分布的碳化物颗粒。