Abstract: A method for reducing the chromium content from a metallurgical slag, in which the slag is charged onto an iron bath in the liquid state and the reduction of Cr is effected by the iron bath having a C content of 2 to 4% by weight, wherein a) the Cr-containing slag having a Cr content of 2 to 20% by weight is charged onto an iron bath having a C content of below 1% by weight, whereupon b) the carbon content of the iron bath is raised to about 2 to 4% by weight by the addition of carbon carriers at the simultaneous supply of energy, c) the liquid slag having a Cr content of about 0.1% by weight is tapped after the reduction of Cr, d) a cooling agent, preferably scrap, is added to the iron melt and the C content of the melt is lowered to below 1% by weight, and e) a portion of the Cr-containing melt is tapped in the liquid state, while the remaining portion is left in the converter in the liquid state for the treatment of the subsequent melt.
Abstract translation: 一种用于将冶金渣中铬含量降低的方法,其中将渣装入液态的铁浴中并且Cr的还原是通过C含量为2至4重量%的铁浴来实现的,其中 a)将Cr含量为2〜20重量%的含Cr矿渣装入C含量低于1重量%的铁浴中,b)将铁浴的碳含量提高到约2 通过在同时供应能量时添加碳载体至4重量%,c)在还原Cr之后,将Cr含量为约0.1重量%的液体渣,d)冷却剂,优选废料, 加入到铁熔体中,并且熔体的C含量降低到低于1重量%,e)一部分含Cr熔体被液化,而其余部分留在转炉中 用于处理后续熔体的液体状态。
-
2.
公开(公告)号:US07641713B2
公开(公告)日:2010-01-05
申请号:US11579102
申请日:2005-05-18
Applicant: Markus Tschudin
Inventor: Markus Tschudin
CPC classification number: C21B3/04 , C21C5/005 , C21C5/36 , C21C7/0025 , C21C2005/5276 , C22B5/10 , C22B7/04 , C22B34/32 , Y02P10/214 , Y02P10/216 , Y02P10/23 , Y02W30/542
Abstract: A method for reducing the chromium content from a metallurgical slag, in which the slag is charged onto an iron bath in the liquid state and the reduction of Cr is effected by the iron bath having a C content of 2 to 4% by weight, wherein a) the Cr-containing slag having a Cr content of 2 to 20% by weight is charged onto an iron bath having a C content of below 1% by weight, whereupon b) the carbon content of the iron bath is raised to about 2 to 4% by weight by the addition of carbon carriers at the simultaneous supply of energy, c) the liquid slag having a Cr content of about 0.1% by weight is tapped after the reduction of Cr, d) a cooling agent, preferably scrap, is added to the iron melt and the C content of the melt is lowered to below 1% by weight, and e) a portion of the Cr-containing melt is tapped in the liquid state, while the remaining portion is left in the converter in the liquid state for the treatment of the subsequent melt.
Abstract translation: 一种用于将冶金渣中铬含量降低的方法,其中将渣装入液态的铁浴中并且Cr的还原是通过C含量为2至4重量%的铁浴来实现的,其中 a)将Cr含量为2〜20重量%的含Cr矿渣装入C含量低于1重量%的铁浴中,b)将铁浴的碳含量提高到约2 通过在同时供应能量时添加碳载体至4重量%,c)在还原Cr之后,将Cr含量为约0.1重量%的液体渣,d)冷却剂,优选废料, 加入到铁熔体中,并且熔体的C含量降低到低于1重量%,e)一部分含Cr熔体被液化,而其余部分留在转炉中 用于处理后续熔体的液体状态。
-