摘要:
An image writing/display device has a voltage applying section, a pressure applying section, an initialization controlling section, and an image writing controlling section. In a state in which a display medium having a pair of electrodes and a display layer that is sandwiched between the pair of electrodes and whose reflectance is changed is positioned, the voltage applying section applies voltage to the pair of electrodes for changing the reflectance of the display layer. The pressure applying section applies pressure for changing the reflectance of the display layer. The initialization controlling section makes the display layer a uniform reflectance by applying pressure to the display layer with the pressure applying section. The image writing controlling section writes an image by applying data voltage from the voltage applying section to specific regions, that correspond to image data, of the display layer between the pair of electrodes.
摘要:
Disclosed is a production apparatus of a wired member, including: a mask forming unit that forms a mask on a transfer substrate by using a toner in accordance with an electrophotographic method so as to be transferable to a member to be wired, the mask corresponding to a wiring pattern to be formed on the member to be wired; a mask transferring unit that transfers the mask formed on the transfer substrate by the toner to the member to be wired; a conductive film forming unit that supplies a conductive material onto the mask-transferred side of the member to be wired to form a film of the conductive material thereon; and a mask removing unit that removes the mask from the member to be wired on which the film of the conductive material has been formed.
摘要:
A baroplastic includes a first resin with a first Tg; and a second resin with a second Tg that is lower than the first Tg by 20° C. or more, and has a photoreactive group.
摘要:
A polyester resin for electrostatic image developing toner includes: two or more polyester blocks, and the polyester resin satisfying the following conditions (A) to (C): (A) an ester concentration of the polyester resin is about 0.01 or more and less than about 0.1; (B) a weight average molecular weight of the polyester resin is about 24,000 or more; and (C) a difference in SP values of at least two kinds of the two or more polyester blocks is about 0.1 to about 0.7.