Method for producing crystalline, inorganic ion exchange material
    1.
    发明授权
    Method for producing crystalline, inorganic ion exchange material 失效
    生产结晶无机离子交换材料的方法

    公开(公告)号:US06027560A

    公开(公告)日:2000-02-22

    申请号:US913634

    申请日:1997-09-19

    CPC分类号: C01B33/36

    摘要: The method for producing a crystalline, inorganic ion exchange material having the following composition: xM.sub.2 O.ySiO.sub.2.zMeO, wherein x, y and z are numerical values satisfying the relationships of y/x=0.5 to 2.1, preferably 0.5 to 2.0, and z/y=0.001 to 1.0; M stands for Na and K, wherein K/Na is in the range from 0.01 to 1.2; and Me stands for Ca and/or Mg, the method including the steps of adding 1 to 85 parts by weight of water to 100 parts by weight of cullets, wherein the cullets have the following compositon: xM.sub.2 O.ySiO.sub.2 .multidot.zMeO, wherein x, y, z, M, and Me are defined as above, and then baking the resulting mixture.

    摘要翻译: PCT No.PCT / JP96 / 00950 Sec。 371日期:1997年9月19日 102(e)1997年9月19日PCT PCT 1996年4月4日PCT公布。 公开号WO96 / 33131 日期:1996年10月24日具有以下组成的结晶无机离子交换材料的制造方法:xM2O.ySiO2.zMeO,其中x,y和z是满足y / x = 0.5〜2.1的关系的数值,优选为0.5 至2.0,z / y = 0.001至1.0; M代表Na和K,其中K / Na在0.01至1.2的范围内; Me表示Ca和/或Mg,该方法包括以下步骤:向100重量份的碎玻璃中加入1至85重量份的水,其中所述碎玻璃具有以下组成:xM2O.ySiO2xzMeO,其中x,y, z,M和Me定义如上,然后烘焙所得混合物。

    Method for producing crystalline, inorganic ion exchange material
    2.
    发明授权
    Method for producing crystalline, inorganic ion exchange material 失效
    生产结晶无机离子交换材料的方法

    公开(公告)号:US5939040A

    公开(公告)日:1999-08-17

    申请号:US894689

    申请日:1997-08-26

    IPC分类号: B01J41/10 C01B33/36 C11D3/08

    CPC分类号: C01B33/36

    摘要: A method for producing a crystalline, inorganic ion exchange material having the following composition: x.sub.1 K.sub.2 O.x.sub.2 Na.sub.2 O.ySiO.sub.2. zMeO, wherein x.sub.1, x.sub.2, y and z are numerical values satisfying the following relationships: y/(x.sub.1 +x.sub.2)=1.0 to 2.1, z/y=0 to 1.0, x.sub.1 /x.sub.2 =0.01 to 2.0, and Me stands for Ca and/or Mg, the method including the steps of adding and blending one or more alkali metal compounds, or one or more alkali metal compounds and one or more alkaline earth metal compounds in cullets having a composition of SiO.sub.2 /Na.sub.2 O=1.5 to 4.2, and baking the resulting mixture.

    摘要翻译: PCT No.PCT / JP96 / 00516 Sec。 371日期:1997年8月26日 102(e)日期1997年8月26日PCT提交1996年3月4日PCT公布。 出版物WO96 / 27555 日本1996年9月12日制备具有以下组成的结晶无机离子交换材料的方法:x1K2O.x2Na2O.ySiO2。 zMeO,其中x1,x2,y和z是满足以下关系的数值:y /(x1 + x2)= 1.0〜2.1,z / y = 0〜1.0,x1 / x2 = 0.01〜2.0,Me表示 Ca和/或Mg的方法,包括以下步骤:在SiO 2 / Na 2 O = 1.5至4.2的碎片中加入和掺混一种或多种碱金属化合物或一种或多种碱金属化合物和一种或多种碱土金属化合物 ,并烘烤得到的混合物。