1.
公开(公告)号:US20160165766A1
公开(公告)日:2016-06-09
申请号:US14558847
申请日:2014-12-03
Inventor: YEN-CHUNG CHEN , SUNG-YING TSAI , HUNG-FANG HUANG , JEN-BING WON , MING-DER GER
IPC: H05K9/00
CPC classification number: H05K9/0081 , B22F9/24 , C22C1/0425 , C22C3/00 , C22C5/06 , C22C9/00 , C22C19/03 , C22C33/02 , C22C38/02 , C22C38/06 , C22C38/16 , H05K9/0083
Abstract: A method for making an electromagnetic wave shielding material comprises the steps of (a) mixing ternary Fe—Al—Si alloy powders and a solvent to prepare a Fe—Al—Si solution; (b) adding an acid in the Fe—Al—Si solution to release Fe ions through a dissolution reaction; (c) adding copper chloride powders in the Fe—Al—Si solution; (d) adding a lye in the Fe—Al—Si solution to induce a displacement reaction; (e) adding a silane coupling agent in the Fe—Al—Si solution; (f) placing the Fe—Al—Si solution in a microwave reactor to accelerate the displacement reaction; (g) producing a quaternary Cu—Fe—Al—Si alloy after the displacement reaction of the Fe—Al—Si solution, thereby forming a quaternary Cu—Fe—Al—Si alloy solution, which proceeding with a solid-liquid separation and a drying treatment to obtain an electromagnetic wave shielding material composed of quaternary Cu—Fe—Al—Si alloy in solid powders.
Abstract translation: 制造电磁波屏蔽材料的方法包括以下步骤:(a)将三元Fe-Al-Si合金粉末和溶剂混合以制备Fe-Al-Si溶液; (b)在Fe-Al-Si溶液中加入酸以通过溶解反应释放Fe离子; (c)在Fe-Al-Si溶液中加入氯化铜粉末; (d)在Fe-Al-Si溶液中加入碱液以引起置换反应; (e)在Fe-Al-Si溶液中加入硅烷偶联剂; (f)将Fe-Al-Si溶液置于微波反应器中以加速置换反应; (g)在Fe-Al-Si溶液置换反应之后生成四价Cu-Fe-Al-Si合金,从而形成一种进行固液分离的四元Cu-Fe-Al-Si合金溶液, 进行干燥处理,得到固体粉末中由四元Cu-Fe-Al-Si合金构成的电磁波屏蔽材料。