Hot-forged TiAl-based alloy and method for producing the same

    公开(公告)号:US10208360B2

    公开(公告)日:2019-02-19

    申请号:US14898257

    申请日:2014-06-02

    Abstract: Provided is a hot-forged TiAl-based alloy of the present invention containing 40 to 45 atom % of Al and additive elements in the following composition ratio (A) or (B), and the balance Ti with inevitable impurities: (A) Nb: 7 to 9 atom %, Cr: 0.4 to 4.0 atom %, Si: 0.3 to 1.0 atom %, and C: 0.3 to 1.0 atom %; and (B) at least one of Cr: 0.1 to 2.0 atom %, Mo: 0.1 to 2.0 atom %, Mn: 0.1 to 4.0 atom %, Nb: 0.1 to 8.0 atom %, and V: 0.1 to 8.0 atom %. The TiAl-based alloy is characterized by having a fine structure of densely arranged lamella grains that are laminated alternately with a Ti3Al phase (α2-phase) and a TiAl phase (γ-phase) and have an average grain size of 1 to 200 μm.

    Hot-forged tial-based alloy, method for producing same, and uses for same

    公开(公告)号:US11920219B2

    公开(公告)日:2024-03-05

    申请号:US17311866

    申请日:2019-12-13

    CPC classification number: C22C14/00 B23P15/02 C22F1/183

    Abstract: The present invention provides a TiAl-based alloy, including: Al: 41 to 43 at %; Fe: 0 to 2.5 at %; Ni: 0 to 2.5 at %; Mo: 0 to 2.0 at %; W: 0 to 2.0 at %; Cr: 0 to 4.5 at %; Mn: 0 to 5.5 at %; V: 0 to 10 at %; Nb: 0 to 10 at %; C: 0.3 to 0.7 at %; and a remainder consisting of Ti and inevitable impurities, in which an alloy element parameter “P=(41.5−Al)/3+Fe+Ni+Mo+W+0.5 Cr+0.4 Mn+0.2 V+0.2 Nb—C” is in a composition range of 1.1 to 1.9, and the TiAl-based alloy has a microstructure consisting of a γ phase of 5 to 30 area %, a β phase of 0.5 to 5 area %, and a lamellar structure occupying a remaining part.

Patent Agency Ranking