Method for manufacturing partially acylated regenerated cellulose foil or fiber
    1.
    发明授权
    Method for manufacturing partially acylated regenerated cellulose foil or fiber 失效
    制备部分再生纤维素纤维素纤维或纤维的方法

    公开(公告)号:US3649341A

    公开(公告)日:1972-03-14

    申请号:US3649341D

    申请日:1968-11-14

    申请人: NESTE OY

    CPC分类号: D06M13/188 C08B1/02 C08B3/06

    摘要: Partly acetylated regenerated cellulose films or fibers are manufactured by first swelling them in a concentrated and waterfree acetic acid solution of an alkali metal acetate at a temperature ranging between 50* and 140* C. Immediately thereafter and without drying the swelled films or fibers are esterified by an acetic acid anhydride solution containing alkali metal acetate at a temperature ranging between 100* and 170* C.