CARBON MATERIAL FOR LITHIUM-ION SECONDARY BATTERY NEGATIVE ELECTRODE, LOW-CRYSTALLINE CARBON IMPREGNATED CARBON MATERIAL FOR LITHIUM-ION SECONDARY BATTERY NEGATIVE ELECTRODE, NEGATIVE ELECTRODE PLATE, AND LITHIUM-ION SECONDARY BATTERY
    1.
    发明申请
    CARBON MATERIAL FOR LITHIUM-ION SECONDARY BATTERY NEGATIVE ELECTRODE, LOW-CRYSTALLINE CARBON IMPREGNATED CARBON MATERIAL FOR LITHIUM-ION SECONDARY BATTERY NEGATIVE ELECTRODE, NEGATIVE ELECTRODE PLATE, AND LITHIUM-ION SECONDARY BATTERY 审中-公开
    用于锂离子二次电池负极电极,负极电极板和锂离子二次电池的低结晶碳碳材料用于锂离子二次电池负极的碳材料

    公开(公告)号:US20090280413A1

    公开(公告)日:2009-11-12

    申请号:US12439311

    申请日:2007-07-06

    IPC分类号: H01M4/58

    摘要: There is obtained a carbon material for lithium-ion secondary battery negative electrode, a low-crystalline carbon impregnated carbon material for lithium-ion secondary battery negative electrode, a negative electrode plate, and a lithium-ion secondary battery, each of which realizes a first charge/discharge cycle with less gas generation and provides a rapid charge/discharge. The carbon material is obtained by: blending and kneading a carbonaceous aggregate with a binder to form a composition; press molding the composition into an article; carbonizing the press molded article; graphitizing the article to obtain an artificial graphite block; milling the block; and carrying out particle size control. The carbon material has characteristics of: (1) R-value=(I1360/I1580)≧0.2, where R-value is defined by the ratio of D band to G band in Raman spectrum using Nd:YAG laser light of 532 nm wavelength; and (2) d(002)≧0.336 nm, and Lc(002)≦50 nm, where d(002) and Lc(002) are crystallographic parameters calculated by Gakushin-method. The carbon material is used for the negative electrode plate of a lithium-ion secondary battery, and used in the lithium-ion secondary battery having therein the negative electrode plate.

    摘要翻译: 得到锂离子二次电池用负极用碳材料,锂离子二次电池用负极用低碳碳浸渍碳材料,负极板,锂离子二次电池,实现了 第一次充放电循环,气体产生较少,并提供快速充放电。 碳材料通过以下方式获得:将碳质骨料与粘合剂混合并捏合以形成组合物; 将组合物压制成制品; 将压制成型品碳化; 石墨化制品以获得人造石墨块; 铣块; 并进行粒度控制。 碳材料具有以下特征:(1)R值=(I1360 / I1580)> = 0.2,其中R值由使用Nd:YAG激光532nm的拉曼光谱中的D带与G带的比率定义 波长; 和(2)d(002)> = 0.336nm,Lc(002)<= 50nm,其中d(002)和Lc(002)是通过Gakushin方法计算的晶体参数。 碳材料用于锂离子二次电池的负极板,并用于其中具有负极板的锂离子二次电池中。