Abstract:
A method is provided for producing a pulverulent precursor material of the general formula M1xM2y(Si,Al)12(O,N)16 or M12-zM2zSi8Al4N16 having the method steps A) producing a pulverulent mixture of starting materials, B) calcining the mixture under a protective gas atmosphere and subsequent grinding, wherein in method step A) at least one nitride with a specific surface area of greater than 2 m2/g is selected as starting material. A pulverulent precursor material and the use thereof are additionally provided.