公开(公告)号:US07758785B2
公开(公告)日:2010-07-20
申请号:US10743562
申请日:2003-12-22
申请人: Renuga Gopal , Kazutoshi Fujihara , Seeram Ramakrishna , Chong-Lin Chew , Ganesh V. Kumar , Kelvin W. C. Foong , Poey-Ling Loh
发明人: Renuga Gopal , Kazutoshi Fujihara , Seeram Ramakrishna , Chong-Lin Chew , Ganesh V. Kumar , Kelvin W. C. Foong , Poey-Ling Loh
CPC分类号: B29C70/44 , B29C70/446 , B29C70/542 , B29C70/56 , B29L2031/7096 , Y10S264/71 , Y10T428/24994
摘要: A fiber reinforced composite is formed using a shrinkable die. A composite of fiber and resin is placed in the die and is compressed by shrinking the die to form a desired transverse cross-section. Optionally, the die is bent along its lengthwise extent to shape the composite in the die. After shrinking and optional shaping, the composite is cured to form the fiber reinforced composite.
摘要翻译: 使用可收缩模具形成纤维增强复合材料。 将纤维和树脂的复合物放置在模具中并通过使模具收缩以形成期望的横截面而被压缩。 可选地,模具沿其纵向方向弯曲以在模具中成形复合材料。 在收缩和任选成型后,复合材料固化形成纤维增强复合材料。