Hydrofluoric acid resistant ceramic mortar
    1.
    发明授权
    Hydrofluoric acid resistant ceramic mortar 失效
    耐氢氟酸陶瓷砂浆

    公开(公告)号:US5932505A

    公开(公告)日:1999-08-03

    申请号:US743163

    申请日:1996-11-04

    IPC分类号: C04B37/00 C04B35/10

    摘要: Hydrofluoric acid-resistant ceramic mortar compositions containing a hydrofluoric acid-resistant grog having a particle size distribution imparting a high particle packing fraction to the mortar composition and a binding phase containing a metal salt having a particle size distribution imparting plasticity to the mortar composition selected from hydrofluoric acid-insoluble fluoride salts, metal salts capable of forming hydrofluoric acid-insoluble fluoride salts upon reaction with a fluorinating reagent and mixtures thereof. Methods for forming hydrofluoric acid-resistant ceramic mortar compositions from non-fluoride metal salts are also disclosed as well as methods for bonding refractory bricks into a brickwork unit with the ceramic mortars of the invention. Brickwork units prepared using the ceramic mortar compositions of the invention by the methods of the invention are also described.

    摘要翻译: 含有赋予砂浆组合物的高粒度填充率的粒度分布的含氢氟酸耐腐蚀砂浆的耐氢氟酸陶瓷砂浆组合物和含有赋予塑性的粒度分布赋予塑性的金属盐的结合相与选自 氢氟酸不溶性氟化物盐,与氟化试剂反应形成氢氟酸不溶性氟化物盐的金属盐及其混合物。 还公开了从非氟化物金属盐形成耐氢氟酸陶瓷砂浆组合物的方法以及将耐火砖粘结到具有本发明的陶瓷砂浆的砖瓦单元中的方法。 还描述了通过本发明的方法使用本发明的陶瓷砂浆组合物制备的砖块单元。

    METHOD OF MANUFACTURING STONE-LIKE ARTICLES
    2.
    发明申请
    METHOD OF MANUFACTURING STONE-LIKE ARTICLES 审中-公开
    制造石头样品的方法

    公开(公告)号:US20080076655A1

    公开(公告)日:2008-03-27

    申请号:US11859324

    申请日:2007-09-21

    IPC分类号: C03C1/02

    CPC分类号: C03C1/06 C03B19/06 C03C1/02

    摘要: A method of manufacturing an article includes granulating glass, clay, filler, and porosity reducing agent to form a mixture, adding binder to the mixture to form granular particles, forming the granular particles into a shaped article by dry pressing, drying the shaped article, and firing the shaped article in a kiln at a maximum temperature of between about 800° C. and about 1100° C. The glass, clay, filler, and porosity reducing agent are granulated in a fluidized bed granulator. Upon addition of the binder, granulated particles are formed having an average particle size of between about 0.08 millimeters and about 5 millimeters. The granular particles comprise between about 55% to about 99% glass by weight, up to about 40% clay by weight, up to about 30% filler by weight, between about 0.1% and about 5% porosity reducing agent by weight, and between about 0.2% and about 3% binder by weight.

    摘要翻译: 制造制品的方法包括将玻璃,粘土,填料和孔隙率降低剂造粒以形成混合物,向混合物中添加粘合剂以形成颗粒状颗粒,通过干压制成型成型制品,干燥成型制品, 并在约800℃至约1100℃的最高温度下在窑中焙烧成型制品。将玻璃,粘土,填料和孔隙率降低剂在流化床造粒机中造粒。 在添加粘合剂时,形成具有约0.08毫米至约5毫米的平均粒度的造粒颗粒。 颗粒颗粒包含按重量计约55%至约99%的玻璃,至多约40%的粘土,至多约30%的填料重量,约0.1%至约5%的孔隙率降低剂,以及在 约0.2%和约3%的粘合剂。