公开(公告)号:US20190380919A1
公开(公告)日:2019-12-19
申请号:US16357399
申请日:2019-03-19
Applicant: SHOFU INC.
Inventor: Shun SHIMOSOYAMA , Katsuya KIMOTO
Abstract: To provide a glass ionomer cement having excellent removality of the surplus cement after curing because of having shape retaining property where a kneaded material does not drip and flow by their own weights, few risk of water sensitivity and excellent operability at the bonding such that surplus cement can be removed easily after an application in an oral cavity in an early timing in spite of exhibiting a thin coating thickness at the bonding. A glass ionomer cement composition for dental luting comprises at least; a component (a) acid reactive glass powder having an average particle diameter within a range of 4.5 to 7.0 μm, a component (b) polymer of an acid group-containing polymerizable monomer having a weight average molecular weight within a range of 30000 to 100000, a component (c) chelating agent and a component (d) water, wherein a plastic flow distance of a kneaded material before curing is 2 mm or less, and a removal possible time of a surplus cement is 2 minutes or less.
-
公开(公告)号:US20240325283A1
公开(公告)日:2024-10-03
申请号:US18618954
申请日:2024-03-27
Applicant: SHOFU INC.
Inventor: Kazuki YAMAMOTO , Shun SHIMOSOYAMA
Abstract: It is an object of the present invention to provide an artificial nail composition having a matte texture with reduced gloss and having high flexibility. The artificial nail composition of the present invention contains a component (A): a polymerizable compound, a component (B): urethane polymer particles, and a component (C): a polymerization initiator.
-
公开(公告)号:US20210212906A1
公开(公告)日:2021-07-15
申请号:US17032212
申请日:2020-09-25
Applicant: SHOFU INC.
Inventor: Shuji SAKAMOTO , Shun SHIMOSOYAMA , Katsuya KIMOTO
Abstract: To provide a dental glass ionomer cement composition which exhibits high mechanical properties. The dental glass ionomer cement composition of the present disclosure comprises
(a) non-crosslinked polyalkenoic acid,
(b) water,
(c) crosslinked polyalkenoic acid: 0.01 to 10 wt. %, and
(d) acid-reactive glass powder.
-
-