COBALT HYDROXIDE PARTICLES AND MANUFACTURING PROCESS THEREFOR AND POSITIVE ELECTRODE ACTIVE MATERIAL AND MANUFACTURING PROCESS THEREFOR
    1.
    发明申请
    COBALT HYDROXIDE PARTICLES AND MANUFACTURING PROCESS THEREFOR AND POSITIVE ELECTRODE ACTIVE MATERIAL AND MANUFACTURING PROCESS THEREFOR 审中-公开
    钴氢氧化物颗粒及其制备方法及其电极活性材料及其制造工艺

    公开(公告)号:US20160308207A1

    公开(公告)日:2016-10-20

    申请号:US15038543

    申请日:2015-01-22

    Abstract: Obtaining cobalt hydroxide particles having a high filling property and a high density. The cobalt hydroxide particles used as a precursor for a positive electrode active material of a non-aqueous electrolyte secondary battery, including spherical secondary particles of flocculated primary particles, wherein average aspect ratio of the secondary particles is 0.7 or more, average particle diameter is 5 to 35 μm, and a value of (d90-d10)/MV indicating a dispersion of a particle size distribution is 0.6 or less, wherein, in sectional observation of the secondary particles, a ratio (N/L) of number (N) of gaps with maximum long diameter 0.3 μm or more recognized in particles of the secondary particles with sectional long diameter 3 μm or more to sectional long diameter (L) of the secondary particles is 1.0 or less, and also, maximum long diameter of the gaps is 15% or less of sectional long diameter of the secondary particles.

    Abstract translation: 获得具有高填充性和高密度的氢氧化钴颗粒。 用作非水电解质二次电池正极活性物质的前体的氢氧化钴粒子,其包含絮凝的一次粒子的球状二次粒子,二次粒子的平均长径比为0.7以上,平均粒径为5 〜35μm,表示粒径分布分散的(d90-d10)/ MV的值为0.6以下,其中,在二次粒子的截面观察中,数(N)的比(N / L) 在二次粒子的截面长径(L)为3倍以上的二次粒子的粒子中,最大长径为0.3μm以上的间隙为1.0以下,间隙的最大长径为 为二次粒子的截面长径的15%以下。