Abstract:
A toner for electrostatic use includes a binder resin including an amorphous polyester resin having a urethane bond and a crystalline polyester resin, a metal ion forming a chemical bond with the binder resin, at least one colorant forming a coordinate bond with the metal ion and being supported on the binder resin through the metal ion, and at least three elements selected from an iron element, a silicon element, a sulfur element, and a fluorine element while including at least one of an iron element, a silicon element, and a sulfur element, wherein an amount of the iron element is about 1000 ppm to about 10000 ppm as an element concentration, an amount of the silicon element is about 1000 ppm to about 5000 ppm as an element concentration, and an amount of the sulfur element is about 500 ppm to about 3000 ppm as an element concentration.
Abstract:
A toner for developing an electrostatic charge image, the toner including: elemental iron, wherein a content of the elemental iron is in a range of 1.0×103 to 1.0×104 ppm, based on a total weight of the toner; elemental silicon, wherein a content of the elemental silicon is in a range of 1.0×103 to 5.0×103 ppm, based on a total weight of the toner; elemental sulfur, wherein a content of the elemental sulfur is in a range of 500 to 3,000 ppm, based on a total weight of the toner; optionally elemental fluorine, wherein a content of the elemental fluorine, if present, is in a range of 1.0×103 to 1.0×104 ppm; and a binder resin
Abstract:
A toner for developing an electrostatic charge image includes three or more elements selected from a group including an iron element, a silicon element, a sulfur element and a fluorine element and a binder resin including an amorphous polyester-based resin.
Abstract:
A toner for developing an electrostatic charge image, the toner including: elemental iron, wherein a content of the elemental iron is in a range of 1.0×103 to 1.0×104 ppm, based on a total weight of the toner; elemental silicon, wherein a content of the elemental silicon is in a range of 1.0×103 to 5.0×103 ppm, based on a total weight of the toner; elemental sulfur, wherein a content of the elemental sulfur is in a range of 500 to 3,000 ppm, based on a total weight of the toner; optionally elemental fluorine, wherein a content of the elemental fluorine, if present, is in a range of 1.0×103 to 1.0×104 ppm; and a binder resin