公开(公告)号:US5597398A
公开(公告)日:1997-01-28
申请号:US260747
申请日:1994-06-15
IPC分类号: C03B37/014 , C03B37/018
CPC分类号: C03B37/0148 , Y02P40/57
摘要: A process for producing a porous glass preform for optical fiber by depositing fine glass particles on an outer surface of a glass material while moving the glass material, including the steps of: preheating a portion of the glass material for not less than 5 minutes to clean the portion of the glass material in an apparatus for depositing fine glass particles; and depositing fine glass particles on the portion of the glass material cleaned by the preheating, in the apparatus for depositing fine glass particles.
摘要翻译: 一种通过在移动玻璃材料的同时在玻璃材料的外表面上沉积微细玻璃颗粒而制造光纤用多孔玻璃预制件的方法,包括以下步骤:将玻璃材料的一部分预热至少5分钟以进行清洁 用于沉积细微玻璃颗粒的装置中的玻璃材料部分; 以及在用于沉积微细玻璃颗粒的装置中,通过预热清洁的玻璃材料的部分上沉积微细玻璃颗粒。