公开(公告)号:US20220037088A1
公开(公告)日:2022-02-03
申请号:US17501817
申请日:2021-10-14
Applicant: TAIYO YUDEN CO., LTD.
Inventor: Chie KAWAMURA , Kazumichi HIROI , Osamu HATTORI
IPC: H01G4/30 , H01G4/12 , C04B35/468 , B32B18/00 , C01G23/00 , C04B35/626
Abstract: A manufacturing method of ceramic powder includes mixing a barium carbonate having a specific surface are of 15 m2/g or more, a titanium dioxide having a specific surface area of 20 m2/g or more, a first compound of a donor element having a larger valence than Ti, and a second compound of an acceptor element having a smaller valence than Ti and having a larger ion radium than Ti and the donor element, and synthesizing barium titanate powder by calcining the barium carbonate, the titanium dioxide, the first compound and the second compound until a specific surface area of the barium titanate powder becomes 4 m2/g or more and 25 m2/g or less.
-
公开(公告)号:US20200286684A1
公开(公告)日:2020-09-10
申请号:US16882342
申请日:2020-05-22
Applicant: TAIYO YUDEN CO., LTD.
Inventor: Chie KAWAMURA , Kazumichi HIROI , Osamu HATTORI
IPC: H01G4/30 , H01G4/12 , C04B35/468 , B32B18/00 , C01G23/00 , C04B35/626
Abstract: A manufacturing method of ceramic powder includes: synthesizing barium titanate powder from barium carbonate, titanium dioxide, manganese carbonate, and one of ammonium molybdate and tungsten oxide, wherein: a solid solution amount of the donor element is 0.05 mol or more and 0.3 mol or less; a solid solution amount of the accepter element with respect to the barium titanate is 0.02 mol or more and 0.2 mol or less on a presumption that the amount of the barium titanate is 100 mol and the acceptor element is converted into an oxide; and relationships y≥−0.0003x+1.0106, y≤−0.0002x+1.0114, 4≤x≤25 and y≤1.0099 are satisfied when a specific surface area of the ceramic powder is “x” and an axial ratio c/a of the ceramic powder is “y”.
-
公开(公告)号:US20190043668A1
公开(公告)日:2019-02-07
申请号:US16155623
申请日:2018-10-09
Applicant: TAIYO YUDEN CO., LTD.
Inventor: Chie KAWAMURA , Kazumichi HIROI , Osamu HATTORI
IPC: H01G4/30 , B32B18/00 , C04B35/468 , H01G4/12 , C04B35/626 , C01G23/00
Abstract: Ceramic powder includes: barium titanate as a main component, wherein: a donor element having a larger valence than Ti is solid-solved in the barium titanate; an acceptor element having a smaller valence than Ti and larger ion radius than Ti and the donor element is solid-solved in the barium titanate, a solid solution amount of the donor element with respect to the barium titanate is 0.05 mol or more and 0.3 mol or less; a solid solution amount of the accepter element with respect to the barium titanate is 0.02 mol or more and 0.2 mol or less; and relationships y≥−0.0003x+1.0106, y≤−0.0002x+1.0114, 4≤x≤25 and y≤1.0099 are satisfied when a specific surface area of the ceramic powder is “x” and an axial ratio c/a of the ceramic powder is “y”.
-
公开(公告)号:US20170372841A1
公开(公告)日:2017-12-28
申请号:US15623253
申请日:2017-06-14
Applicant: TAIYO YUDEN CO., LTD.
Inventor: Chie KAWAMURA , Kazumichi HIROI , Osamu HATTORI
IPC: H01G4/30 , C04B35/468 , H01G4/12
CPC classification number: H01G4/30 , B32B18/00 , C01G23/006 , C01P2002/34 , C01P2002/50 , C01P2002/72 , C01P2002/88 , C01P2006/12 , C04B35/4682 , C04B35/62655 , C04B35/62685 , C04B2235/3224 , C04B2235/3239 , C04B2235/3256 , C04B2235/3258 , C04B2235/3262 , C04B2235/3267 , C04B2235/3418 , C04B2235/5296 , C04B2235/5409 , C04B2235/663 , C04B2237/346 , C04B2237/68 , H01G4/1218 , H01G4/1227
Abstract: A multilayer ceramic capacitor includes: a multilayer structure in which ceramic dielectric layers and internal electrode layers are alternately stacked, wherein: a main component of the ceramic dielectric layer is barium titanate in which a donor element having a larger valence than Ti is solid-solved and an acceptor element having a smaller valence than Ti and larger ion radius than Ti and the donor element is solid-solved; a solid-solution amount of the donor element is 0.05 mol or more and 0.3 mol or less on a presumption that an amount of the barium titanate is 100 mol and the donor element is converted into an oxide; and a solid solution amount of the accepter element is 0.02 mol or more and 0.2 mol or less on a presumption that the amount of the barium titanate is 100 mol and the acceptor element is converted into an oxide.
-
-
-