公开(公告)号:US20230383123A1
公开(公告)日:2023-11-30
申请号:US18247221
申请日:2021-09-29
发明人: Kazutake MORITA , Toshihiro TANAKA
CPC分类号: C08L75/08 , C08G18/7671 , C08G18/4854 , C08L2205/025 , C08L2203/12
摘要: Problem To provide a polyurethane elastic yarn having good heat setting properties in a wide temperature range and high thermal adhesive strength in a wide temperature range while also maintaining its elastic properties (permanent deformation and elongation). Solution A polyurethane elastic yarn comprising polyurethane polymer [A] and polyurethane polymer [B] below, wherein the ratio of polyurethane polymer [A] to polyurethane polymer [B] in terms of parts by mass is from 1:99 to 30:70 or from 70:30 to 99:1, the exothermic peak (crystallization peak) of the polyurethane elastic yarn as measured by a differential scanning calorimeter (DSC) is in the range from 110° C. to 210° C., and the heat capacity at the exothermic peak is 3.0 J/g or more and 100 J/g or less. Polyurethane polymer [A]: a polyurethane polymer using as starting materials polymer diol A whose main chain repeating unit is an ether or an ester, diisocyanate A whose main skeleton is aromatic or aliphatic, and a single low molecular weight diol A having from 2 to 4 carbon atoms CA serving as a chain extender. Polyurethane polymer [B]: a polyurethane polymer using as starting materials polymer diol A, diisocyanate A, and a single low molecular weight diol B having from 1 to 4 carbon atoms CB more than CA serving as a chain extender.