Heat-resistant multilayer container and method for producing the same

    公开(公告)号:US11148402B2

    公开(公告)日:2021-10-19

    申请号:US17269379

    申请日:2019-08-30

    Abstract: A multilayer container including: an outermost layer (1) containing a propylene-based polymer A containing homopolypropylene as a main component having a melt flow rate in a range of 2.0 to 10.0 g/10 min; an inner layer (2) containing 50 to 99% by weight of a propylene-based polymer B containing homopolypropylene as a main component having a melt flow rate of not more than 5.0 g/10 min and an isotactic index of not less than 93%, and 1 to 50% by weight of an ethylene-α-olefin copolymer C; and a barrier layer (4) occupying 5 to 20% by weight of the whole container. The ratio (L/D) of container height (L) to diameter (D) is not less than 0.5, and a volume shrinkage based on volume measured before and after heat sterilization at 121° C. for 30 minutes is not more than 5%.

    MULTILAYERED CONTAINER
    2.
    发明申请
    MULTILAYERED CONTAINER 审中-公开
    多层容器

    公开(公告)号:US20150251390A1

    公开(公告)日:2015-09-10

    申请号:US14430328

    申请日:2013-09-27

    Abstract: A multilayered container includes at least a polyolefin inner layer; an adhesive layer; a gas-barrier layer; an oxygen-absorbing layer; a gas-barrier layer; an adhesive layer; a polyolefin outer layer, and having at least a body portion and a bottom portion, wherein the gas-barrier layers include an ethylene-vinyl alcohol copolymer, the oxygen-absorbing layer includes an oxygen-absorbing resin composition that contains the ethylene-vinyl alcohol copolymer and an oxidizing organic component, an adsorbing agent is contained on the side inside of said gas-barrier layer, the thickness of the multilayered container at the thinnest portion is not more than 430 μm, and the amount of oxygen absorbed after the heat-sterilization is not less than 23 cc per gram of the oxygen-absorbing resin composition. Despite of this decreased thickness, the multilayered container maintains excellent oxygen-barrier property and property for retaining flavor of the content even when it is subjected to the retort sterilization.

    Abstract translation: 多层容器至少包括聚烯烃内层; 粘合层; 阻气层; 氧吸收层; 阻气层; 粘合层; 聚烯烃外层,并且至少具有主体部分和底部部分,其中阻气层包括乙烯 - 乙烯醇共聚物,氧吸收层包括含有乙烯 - 乙烯醇的氧吸收树脂组合物 共聚物和氧化性有机成分,所述阻气层的内侧含有吸附剂,最薄部的多层容器的厚度为430μm以下, 每克氧吸收树脂组合物的灭菌不小于23cc。 尽管厚度减小,但是即使进行蒸煮灭菌,多层容器也保持优异的氧气阻隔性和用于保持内含物质的性能。

    Multilayered containers
    3.
    发明授权

    公开(公告)号:US11298926B2

    公开(公告)日:2022-04-12

    申请号:US16493196

    申请日:2018-03-14

    Abstract: A gas-barrier multilayered container having (i) a layer of a propylene type polymer which chiefly includes a homopolypropylene having an isotactic index of not less than 93%, and (ii) a layer of an ethylene-vinyl alcohol copolymer having not less than two crystal melting peak temperatures. Also disclosed is a lustrous and shock-resistant multilayered container having at least (i) an outermost layer of a propylene type polymer A which chiefly includes a homopolypropylene having a melt flow rate of 2.0 to 10.0 g/10 min., and (ii) an inner layer of a propylene type polymer B which chiefly includes a homopolypropylene having a melt flow rate of not more than 1.0 g/10 min.

    Multilayered container
    4.
    发明授权

    公开(公告)号:US10213991B2

    公开(公告)日:2019-02-26

    申请号:US14430328

    申请日:2013-09-27

    Abstract: A multilayered container includes at least a polyolefin inner layer; an adhesive layer; a gas-barrier layer; an oxygen-absorbing layer; a gas-barrier layer; an adhesive layer; a polyolefin outer layer, and having at least a body portion and a bottom portion, wherein the gas-barrier layers include an ethylene-vinyl alcohol copolymer, the oxygen-absorbing layer includes an oxygen-absorbing resin composition that contains the ethylene-vinyl alcohol copolymer and an oxidizing organic component, an adsorbing agent is contained on the side inside of said gas-barrier layer, the thickness of the multilayered container at the thinnest portion is not more than 430 μm, and the amount of oxygen absorbed after the heat-sterilization is not less than 23 cc per gram of the oxygen-absorbing resin composition. Despite of this decreased thickness, the multilayered container maintains excellent oxygen-barrier property and property for retaining flavor of the content even when it is subjected to the retort sterilization.