公开(公告)号:US20150368731A1
公开(公告)日:2015-12-24
申请号:US14769564
申请日:2014-02-25
Applicant: TOYO TANSO CO., LTD.
Inventor: Shingo Bito , Yuji Tomita , Yuji Fujioka , Syuhei Tomita , Hiroshi Machino
CPC classification number: C21D1/63 , C04B35/521 , C04B35/83 , C04B41/83 , C04B41/87 , C04B2235/77 , C21D1/00 , C21D1/58 , C21D9/0025
Abstract: A purpose is to provide a tray for oil quenching heat treatment furnaces that can inhibit oil infiltration to reduce adverse effects on the quality of the workpiece and also can make lightweight design of the tray possible.Provided is a tray including a carbon material and being capable of placing a workpiece thereon for oil quenching of the workpiece, characterized in that the cumulative pore volume of pores with a pore radius of greater than or equal to 1 μm is less than or equal to 40 mm3/g in the carbon material. The carbon material is desirably such that a C/C composite is impregnated with a thermosetting resin and burned.
Abstract translation: 目的是提供一种用于油淬火热处理炉的托盘,其能够抑制油渗入以减少对工件质量的不利影响,并且还可以使得托盘的轻量化设计成为可能。 提供一种包括碳材料的托盘,其能够在其上放置工件用于工件的油淬,其特征在于,孔半径大于或等于1μm的孔的累积孔体积小于或等于 40 mm3 / g的碳材料。 碳材料优选使得C / C复合材料用热固性树脂浸渍并烧制。
-
公开(公告)号:US10718569B2
公开(公告)日:2020-07-21
申请号:US14896027
申请日:2014-06-04
Applicant: TOYO TANSO CO., LTD.
Inventor: Syuhei Tomita , Hiroshi Machino , Toshiharu Hiraoka , Shingo Bito
IPC: F27D5/00 , D03D15/12 , F27D3/02 , D03D1/00 , D03D13/00 , D03D19/00 , C21D9/00 , F27D3/12 , F27D3/00
Abstract: The present invention improves the strength of the bottom (net) of the jig and makes it more difficult and unlikely for deviation of the mesh to occur.A workpiece is loaded on the net (2) of the heat treat furnace jig (hereinafter, heat treatment furnace jig). In the net (2), a first strand (10), a second strand (20) and a third strand (30) are in contact at a contact point (X1). Near the contact point (X1), the second strand (20) overlaps the first strand (10) from above and the third strand (30) overlaps the first strand (10) from below. As a result, the first strand (10) is held between the second strand (20) and the third strand (30) in the up/down directions.
-
公开(公告)号:US20160123670A1
公开(公告)日:2016-05-05
申请号:US14896027
申请日:2014-06-04
Applicant: TOYO TANSO CO., LTD.
Inventor: Syuhei Tomita , Hiroshi Machino , Toshiharu Hiraoka , Shingo Bito
Abstract: The present invention improves the strength of the bottom (net) of the jig and makes it more difficult and unlikely for deviation of the mesh to occur.A workpiece is loaded on the net (2) of the heat treat furnace jig (hereinafter, heat treatment furnace jig). In the net (2), a first strand (10), a second strand (20) and a third strand (30) are in contact at a contact point (X1). Near the contact point (X1), the second strand (20) overlaps the first strand (10) from above and the third strand (30) overlaps the first strand (10) from below. As a result, the first strand (10) is held between the second strand (20) and the third strand (30) in the up/down directions.
Abstract translation: 本发明提高了夹具的底部(网)的强度,并且使得网格的偏移发生变得困难且不太可能。 将工件装载在热处理炉夹具(以下称为热处理炉夹具)的网(2)上。 在网(2)中,第一股(10),第二股(20)和第三股(30)在接触点(X1)处接触。 在接触点(X1)附近,第二股线(20)从上方与第一股线(10)重叠,第三股线(30)从下方与第一股线(10)重叠。 结果,第一股线(10)在上/下方向上保持在第二股线(20)和第三股线(30)之间。
-
公开(公告)号:US20150136017A1
公开(公告)日:2015-05-21
申请号:US14411182
申请日:2013-07-01
Applicant: TOYO TANSO CO., LTD.
Inventor: Toshiharu Hiraoka , Hiroshi Machino , Masaaki Kawakami
CPC classification number: C30B15/10 , C30B29/06 , C30B35/002 , Y10T29/49826 , Y10T117/1032
Abstract: A carbon crucible (1) has a structure including a straight trunk portion (9) and a tray portion (10) vertically separated from each other. The straight trunk portion (9) is made of a carbon fiber-reinforced carbon composite material and the tray portion (10) is made of graphite. An upper end face of the tray portion (9) is provided with a step portion (11) having an outer circumference-side region that is higher relative to an inner circumference-side region thereof. The straight trunk portion (9) is fitted to the step portion (11), and in the straight trunk portion (9) and the step portion (9) that are fitted to each other, a gap is provided between an inner circumferential surface (11a) of the step portion (11) and an outer circumferential surface (9a) of the straight trunk portion (9). The gap is preferably from 0.1% to 1.0% of the diameter of the straight trunk portion.
Abstract translation: 碳坩埚(1)具有直立躯干部(9)和垂直分离的托盘部(10)的结构。 直的躯干部分(9)由碳纤维增强碳复合材料制成,托盘部分(10)由石墨制成。 托盘部(9)的上端面设置有具有相对于其内周侧区域高的外周侧区域的台阶部(11)。 直的躯干部(9)嵌合在台阶部(11)上,并且在相互嵌合的直线主干部(9)和台阶部(9)中,在内周面 (11)的外周面(9a)和直线躯干部(9)的外周面(9a)之间。 该间隙优选为直的躯干部的直径的0.1%至1.0%。
-
-
-