Abstract:
A porous carbon having a high oxidation reaction temperature, a method of manufacturing the porous carbon, and an adsorption/desorption apparatus using the porous carbon are provided. A porous carbon includes mesopores and a carbonaceous wall forming an outer wall of the mesopores, characterized by being composed mainly of hard carbon and having an oxidation reaction temperature of 600° C. or higher. It is desirable that the porous carbon have an average interlayer spacing d(002) of 0.350 nm or greater, as determined by an X-ray diffraction method after heating the porous carbon at 2500° C. or higher for 30 minutes to 60 minutes.