Developing roller and imaging apparatus comprising the same
    1.
    发明授权
    Developing roller and imaging apparatus comprising the same 有权
    显影辊和包括其的成像装置

    公开(公告)号:US08550968B2

    公开(公告)日:2013-10-08

    申请号:US11594120

    申请日:2006-11-08

    IPC分类号: F16C13/00

    CPC分类号: G03G15/0818

    摘要: There is a developing roller having a low compression permanent strain without contaminating a photosensitive drum and deteriorating toners. The developing roller 1 comprises a shaft 2, an elastic layer 3 formed on an outer periphery of the shaft 2 and a surface coating layer 4 formed on an outer peripheral face of the elastic layer 3, in which the surface coating layer 4 comprises a urethane resin formed by crosslinking a lactone-modified polyol with a polyisocyanate. The urethane resin is preferable to be formed by crosslinking the lactone-modified polyol with two or more kinds of polyisocyanates.

    摘要翻译: 存在具有低压缩永久应变而不污染感光鼓并劣化调色剂的显影辊。 显影辊1包括轴2,形成在轴2的外周上的弹性层3和形成在弹性层3的外周面上的表面涂层4,其中表面涂层4包括聚氨酯 通过将内酯改性的多元醇与多异氰酸酯交联而形成的树脂。 聚氨酯树脂优选通过将内酯改性的多元醇与两种以上的多异氰酸酯交联而形成。

    Developing roller and imaging apparatus comprising the same
    2.
    发明申请
    Developing roller and imaging apparatus comprising the same 有权
    显影辊和包括其的成像装置

    公开(公告)号:US20070111874A1

    公开(公告)日:2007-05-17

    申请号:US11594120

    申请日:2006-11-08

    IPC分类号: F16C13/00

    CPC分类号: G03G15/0818

    摘要: There is a developing roller having a low compression permanent strain without contaminating a photosensitive drum and deteriorating toners. The developing roller 1 comprises a shaft 2, an elastic layer 3 formed on an outer periphery of the shaft 2 and a surface coating layer 4 formed on an outer peripheral face of the elastic layer 3, in which the surface coating layer 4 comprises a urethane resin formed by crosslinking a lactone-modified polyol with a polyisocyanate. The urethane resin is preferable to be formed by crosslinking the lactone-modified polyol with two or more kinds of polyisocyanates.

    摘要翻译: 存在具有低压缩永久应变而不污染感光鼓并劣化调色剂的显影辊。 显影辊1包括轴2,形成在轴2的外周上的弹性层3和形成在弹性层3的外周面上的表面涂层4,其中表面涂层4包括聚氨酯 通过将内酯改性的多元醇与多异氰酸酯交联而形成的树脂。 聚氨酯树脂优选通过将内酯改性的多元醇与两种以上的多异氰酸酯交联而形成。