Polyolefin resin pre-expanded particles and process for preparing the same

    公开(公告)号:US06593382B2

    公开(公告)日:2003-07-15

    申请号:US10058077

    申请日:2002-01-29

    IPC分类号: C08J918

    CPC分类号: C08J9/18 C08J2323/02

    摘要: Polyolefin resin pre-expanded particles having two fusion peaks on DSC curve wherein the proportion of the heat of fusion Qh of the peak appearing on the high temperature side based on the total heat of fusion of the two peaks represented by the equation: [Qh/(Ql+Qh)]×100 falls within the range of 10 to 60% in which Ql is the heat of fusion of the peak appearing on the low temperature side, and the standard deviation of said proportion is not more than 1.2. The pre-expanded particles are prepared by releasing an aqueous dispersion of resin particles impregnated with a blowing agent from a vessel into an atmosphere of lower pressure than the inner pressure of the vessel to expand the particles, while stepwise or continuously raising the inner temperature or the inner pressure of the vessel at a specific rate, and can be molded with stable molding cycle to give cellular molded articles having stable dimensions.

    Polypropylene Resin Pre-Expanded Particles And In-Mold Foamed Articles Prepared Therefrom
    2.
    发明申请
    Polypropylene Resin Pre-Expanded Particles And In-Mold Foamed Articles Prepared Therefrom 有权
    聚丙烯树脂预发泡颗粒和在其中制备的模内发泡制品

    公开(公告)号:US20080153933A1

    公开(公告)日:2008-06-26

    申请号:US11795067

    申请日:2005-12-21

    IPC分类号: C08F210/06

    摘要: An object of the present invention is to provide an in-mold foamed article having good surface appearances and high rigidity produced by using a common molding machine that withstands a pressure of up to 0.4 MPa. The present invention provides polypropylene resin pre-expanded particles containing a base resin which is a resin having a melt flow rate of 5 g/10 min or more and 20 g/10 min or less and a melting point of 140° C. or higher and 155° C. or lower and satisfying the conditional formula below, and an in-mold foamed article produced from molding the pre-expanded particles: [Heat of crystal fusion (J/g)]≧1.2×[Melting point (° C.)]−96

    摘要翻译: 本发明的目的是提供一种具有良好的表面外观和高刚性的模内发泡制品,其通过使用耐受高达0.4MPa的压力的普通成型机。 本发明提供聚丙烯树脂预发泡粒子,其含有熔体流动速率为5g / 10分钟以上且20g / 10分钟以下且熔点为140℃以上的树脂的基础树脂 和155℃以下,满足下述条件式,以及通过模制预发泡颗粒而制造的模内发泡制品:<?in-line-formula description =“In-line Formulas”end =“lead” α> [晶体熔化热(J / g)]> = 1.2×[熔点(℃)] - 96 <?在线公式描述=“在线公式”end =“tail”

    Polypropylene resin pre-expanded particles and in-mold foamed articles prepared therefrom
    3.
    发明授权
    Polypropylene resin pre-expanded particles and in-mold foamed articles prepared therefrom 有权
    聚丙烯树脂预发泡颗粒和由其制备的模内发泡制品

    公开(公告)号:US08569390B2

    公开(公告)日:2013-10-29

    申请号:US11795067

    申请日:2005-12-21

    IPC分类号: C08J9/16 C08J9/22 C08L23/00

    摘要: An object of the present invention is to provide an in-mold foamed article having good surface appearances and high rigidity produced by using a common molding machine that withstands a pressure of up to 0.4 MPa. The present invention provides polypropylene resin pre-expanded particles containing a base resin which is a resin having a melt flow rate of 5 g/10 min or more and 20 g/10 min or less and a melting point of 140° C. or higher and 155° C. or lower and satisfying the conditional formula below, and an in-mold foamed article produced from molding the pre-expanded particles: [Heat of crystal fusion (J/g)]≧1.2×[Melting point (° C.)]−96.

    摘要翻译: 本发明的目的是提供一种具有良好的表面外观和高刚性的模内发泡制品,其通过使用耐受高达0.4MPa的压力的普通成型机。 本发明提供聚丙烯树脂预发泡粒子,其含有熔体流动速率为5g / 10分钟以上且20g / 10分钟以下且熔点为140℃以上的树脂的基础树脂 155℃以下,满足下述条件式,通过模塑预发泡粒子制成的模内发泡体:[结晶熔化热(J / g)]> = 1.2×[熔点(° C)] - 96。

    Collision energy-absorbing material for vehicle and collision energy-absorbing structure of vehicle using the material
    4.
    发明申请
    Collision energy-absorbing material for vehicle and collision energy-absorbing structure of vehicle using the material 审中-公开
    车辆碰撞能量吸收材料和使用该材料的车辆碰撞能量吸收结构

    公开(公告)号:US20060145490A1

    公开(公告)日:2006-07-06

    申请号:US10524776

    申请日:2003-08-27

    IPC分类号: B60R19/18

    摘要: There are provided a vehicle impact energy absorbing member which is arranged as an impact energy absorbing member of a simple construction capable of absorbing impact energy with high efficiency, and which is capable of improving the pedestrian protection performance as well as the passenger protection performance, and a vehicle impact energy absorbing structure using the vehicle impact energy absorbing member. More specifically, a compression energy absorbing member 10 using compression deformation and a buckling energy absorbing member 20 using buckling deformation are provided. Impact energy applied to a vehicle body is absorbed by a combination of the two energy absorbing members 10 and 20. Buckling energy absorbing portions 11a and 11b are also provided which have a buckling characteristic such that a peak value of impact force is equal to or smaller than a set value and in which a setting is made such that at least one of impact timing for starting absorption of impact energy and peak value timing for making the impact force have a peak value after collision is changed in a stepping manner or continuously. Impact energy applied to the vehicle body is absorbed by buckling deformation of the buckling energy absorbing portions 11a and 11b.

    摘要翻译: 提供了一种车辆冲击能量吸收构件,其被布置为能够以高效率吸收冲击能量的简单结构的冲击能量吸收构件,并且能够改善行人保护性能以及乘客保护性能,以及 使用车辆冲击能量吸收构件的车辆冲击能量吸收结构。 更具体地,提供使用压缩变形的压缩能量吸收构件10和使用屈曲变形的屈曲能量吸收构件20。 施加到车体的冲击能量被两个能量吸收构件10和20的组合吸收。 还提供了弯曲能量吸收部分11a和11b,其具有使冲击力的峰值等于或小于设定值的弯曲特性,并且其中设置使得至少一个冲击正时为 冲击力的开始吸收和使冲击力具有碰撞后的峰值的峰值时间以步进方式或连续地改变。 施加到车体的冲击能量被屈曲能量吸收部分11a和11b的屈曲变形所吸收。

    Pre-expanded polypropylene resin beads and process for producing same
    5.
    发明授权
    Pre-expanded polypropylene resin beads and process for producing same 有权
    预发泡聚丙烯树脂珠及其制备方法

    公开(公告)号:US08785508B2

    公开(公告)日:2014-07-22

    申请号:US13377848

    申请日:2010-06-17

    申请人: Taro Kiguchi

    发明人: Taro Kiguchi

    IPC分类号: C08J9/08 C08J9/228

    摘要: The present invention provides pre-expanded polypropylene resin beads comprising (A) a glycerin monoester of a C6 to C24 fatty acid and/or a polyglycerin monoester of a C6 to C24 fatty acid and (B) a glycerin diester of a C6 to C24 fatty acid(s) and/or a polyglycerin diester of a C6 to C24 fatty acid(s), in such a manner that a weight ratio [=(A)/(B)] between (A) and (B) in the polypropylene resin particles is 1.3 or more but 10 or less, and a total content [=(A)+(B)] is 0.3 parts by weight or more but 5 parts by weight or less with respect to 100 parts by weight of the polypropylene resin. The resin particles can be excellently used in in-mold foaming, without requiring washing with a chemical like nitric acid or metaphosphate soda, and can provide a polypropylene resin in-mold foamed product with good antistatic properties.

    摘要翻译: 本发明提供了预发泡聚丙烯树脂珠粒,其包含(A)C6至C24脂肪酸的甘油单酯和/或C6至C24脂肪酸的聚甘油单酯和(B)C6至C24脂肪酸的甘油二酯 (C)和(B)的重量比[=(A)/(B)]在聚丙烯中的重量比[=(A)/(B)] 树脂粒子为1.3以上10以下,相对于100重量份的聚丙烯树脂,总含量[=(A)+(B)]为0.3重量份以上且5重量份以下 。 树脂颗粒可以非常好地用于模内发泡,而不需要用诸如硝酸或偏磷酸钠的化学品洗涤,并且可以提供具有良好抗静电性能的聚丙烯树脂模内发泡产品。

    PRE-EXPANDED POLYPROPYLENE RESIN BEADS AND PROCESS FOR PRODUCING SAME
    6.
    发明申请
    PRE-EXPANDED POLYPROPYLENE RESIN BEADS AND PROCESS FOR PRODUCING SAME 有权
    预扩展的聚丙烯树脂珠及其生产方法

    公开(公告)号:US20120088854A1

    公开(公告)日:2012-04-12

    申请号:US13377848

    申请日:2010-06-17

    申请人: Taro Kiguchi

    发明人: Taro Kiguchi

    摘要: The present invention provides pre-expanded polypropylene resin beads comprising (A) a glycerin monoester of a C6 to C24 fatty acid and/or a polyglycerin monoester of a C6 to C24 fatty acid and (B) a glycerin diester of a C6 to C24 fatty acid(s) and/or a polyglycerin diester of a C6 to C24 fatty acid(s), in such a manner that a weight ratio [=(A)/(B)] between (A) and (B) in the polypropylene resin particles is 1.3 or more but 10 or less, and a total content [=(A)+(B)] is 0.3 parts by weight or more but 5 parts by weight or less with respect to 100 parts by weight of the polypropylene resin. The resin particles can be excellently used in in-mold foaming, without requiring washing with a chemical like nitric acid or methaphosphate soda, and can provide a polypropylene resin in-mold foamed product with good antistatic properties.

    摘要翻译: 本发明提供了预发泡聚丙烯树脂珠粒,其包含(A)C6至C24脂肪酸的甘油单酯和/或C6至C24脂肪酸的聚甘油单酯和(B)C6至C24脂肪酸的甘油二酯 (C)和(B)的重量比[=(A)/(B)]在聚丙烯中的重量比[=(A)/(B)] 树脂粒子为1.3以上10以下,相对于100重量份的聚丙烯树脂,总含量[=(A)+(B)]为0.3重量份以上且5重量份以下 。 树脂颗粒可以非常适用于模内发泡,而不需要用诸如硝酸或甲基磷酸钠的化学品洗涤,并且可以提供具有良好抗静电性能的聚丙烯树脂模内发泡产品。