Coal liquefaction process
    2.
    发明授权
    Coal liquefaction process 失效
    煤液化过程

    公开(公告)号:US4437974A

    公开(公告)日:1984-03-20

    申请号:US389566

    申请日:1982-06-17

    CPC分类号: C10G1/083 C10G1/006

    摘要: A coal liquefaction process and apparatus therefor are disclosed. According to this invention, a finely divided coal and a solvent are contacted with molecular hydrogen in the presence of a catalyst to provide a slurry, the slurry is separated into a gaseous component, a liquid component and a solid residue, the solid residue which is the liquefaction residue is then supplied to a molten metal bath together with oxygen gas to generate a gas entraining fine powdery solids, and the thus recovered fine powdery solids are returned to the liquefaction process as a catalyst.

    摘要翻译: 公开了一种煤液化方法及其设备。 根据本发明,细碎的煤和溶剂在催化剂的存在下与分子氢接触以提供浆料,将浆料分离成气体组分,液体组分和固体残余物,固体残余物是 然后将液化残余物与氧气一起供应到熔融金属浴中,以产生夹带细粉末状固体的气体,将回收的细粉末固体作为催化剂返回到液化过程。

    Method for the preparation of naphthoquinone
    3.
    发明授权
    Method for the preparation of naphthoquinone 失效
    萘醌的制备方法

    公开(公告)号:US4960914A

    公开(公告)日:1990-10-02

    申请号:US300695

    申请日:1989-01-19

    申请人: Ryohei Minami

    发明人: Ryohei Minami

    摘要: A catalyst for use in vapor phase oxidation of naphthalene into 1,4-naphthoquinone is dislosed. The catalyst which is supported on an inert carrier material is represented by the formula:(V)a(K)b(S)c(Fe)d(Sn)e(X)f(O)gwhere V, K, S, Fe, Sn and O stand for vanadium, potassium, sulfur, iron, tin and oxygen, respectively; X stands for at least one element such as silicon, titanium or aluminum which serves as a carrier in the form of oxide; and a, b, c, d, e, f and g are the atomic fractions of the respective elements wherein the ratio of a:b:c:d:e:f=10:10-100:5-100:0.1-10:0.05-10:10-300. Using the above catalyst the vapor phase oxidation can be effected at a relatively low temperature of not higher than 500.degree. C., usually not higher than 420.degree. C., resulting in the formation of 1,4-naphthoquinone in a high yield and with a high selectivity.

    摘要翻译: 用于将萘气相氧化成1,4-萘醌的催化剂被封闭。 负载在惰性载体材料上的催化剂由下式表示:(V)a(K)b(S)c(Fe)d(Sn)e(X)f(O)g其中V,K,S ,Fe,Sn和O分别代表钒,钾,硫,铁,锡和氧; X表示作为氧化物形式的载体的至少一种元素,例如硅,钛或铝; a:b:c:d:e:f = 10:10:100:5-100:0.1〜 10:0.05-10:10-300。 使用上述催化剂,气相氧化可以在不高于500℃,通常不高于420℃的相对低的温度下进行,导致以高产率形成1,4-萘醌,并且与 高选择性。