Adjusting yield of a manufacturing process for energetic compounds through solubility modification
    1.
    发明授权
    Adjusting yield of a manufacturing process for energetic compounds through solubility modification 有权
    通过溶解度改性调整高能化合物的制造工艺的产量

    公开(公告)号:US08002917B2

    公开(公告)日:2011-08-23

    申请号:US12367562

    申请日:2009-02-09

    IPC分类号: C06B25/34 D03D23/00

    CPC分类号: C06B21/0091 C06B25/34

    摘要: A method of adjusting the yield of a manufactured compound comprising primarily two energetic materials to yield a product comprising primarily one of the two energetic materials. Specifically, embodiments of the present invention provide a method of purifying a compound primarily comprising RDX and HMX to achieve a desired purity of RDX with an acceptable yield percentage. By adding sufficient acetonitrile (ACN) to the manufactured compound to dissolve it and form a solution; adding a pre-specified volume of water to the resultant solution and stirring sufficiently to precipitate at least the RDX; separating and drying the precipitate, a pre-specified purity and yield percentage of RDX may be obtained by varying the volume of water added. The process uses relatively environmentally benign recyclable solvents at ambient temperature and pressure reducing both environmental impact and energy costs.

    摘要翻译: 调整主要包含两种能量材料的制造化合物的产率的方法,以产生主要包含两种能量材料中的一种的产品。 具体地,本发明的实施方案提供了一种纯化主要包含RDX和HMX的化合物以获得具有可接受的产率百分比的所需纯度的RDX的方法。 通过向制备的化合物中加入足够的乙腈(ACN)使其溶解并形成溶液; 向所得溶液中加入预定体积的水并充分搅拌至少沉淀RDX; 分离和干燥沉淀物,可以通过改变添加的水的体积来获得RDX的预先规定的纯度和产率百分比。 该方法在环境温度和压力下使用相对环境友好的可回收溶剂,降低了环境影响和能源成本。

    ADJUSTING YIELD OF A MANUFACTURING PROCESS FOR ENERGETIC COMPOUNDS THROUGH SOLUBILITY MODIFICATION
    2.
    发明申请
    ADJUSTING YIELD OF A MANUFACTURING PROCESS FOR ENERGETIC COMPOUNDS THROUGH SOLUBILITY MODIFICATION 有权
    通过可溶性改性调整能量化合物的制造工艺

    公开(公告)号:US20100200128A1

    公开(公告)日:2010-08-12

    申请号:US12367562

    申请日:2009-02-09

    IPC分类号: C06B25/34

    CPC分类号: C06B21/0091 C06B25/34

    摘要: A method of adjusting the yield of a manufactured compound comprising primarily two energetic materials to yield a product comprising primarily one of the two energetic materials. Specifically, embodiments of the present invention provide a method of purifying a compound primarily comprising RDX and HMX to achieve a desired purity of RDX with an acceptable yield percentage. By adding sufficient acetonitrile (ACN) to the manufactured compound to dissolve it and form a solution; adding a pre-specified volume of water to the resultant solution and stirring sufficiently to precipitate at least the RDX; separating and drying the precipitate, a pre-specified purity and yield percentage of RDX may be obtained by varying the volume of water added. The process uses relatively environmentally benign recyclable solvents at ambient temperature and pressure reducing both environmental impact and energy costs.

    摘要翻译: 调整主要包含两种能量材料的制造化合物的产率的方法,以产生主要包含两种能量材料中的一种的产品。 具体地,本发明的实施方案提供了一种纯化主要包含RDX和HMX的化合物以获得具有可接受的产率百分比的所需纯度的RDX的方法。 通过向制备的化合物中加入足够的乙腈(ACN)使其溶解并形成溶液; 向所得溶液中加入预定体积的水并充分搅拌至少沉淀RDX; 分离和干燥沉淀物,可以通过改变添加的水的体积来获得RDX的预先规定的纯度和产率百分比。 该方法在环境温度和压力下使用相对环境友好的可回收溶剂,降低了环境影响和能源成本。