公开(公告)号:US20040177722A1
公开(公告)日:2004-09-16
申请号:US10787085
申请日:2004-02-27
IPC分类号: C22B001/24
CPC分类号: C22B1/2406 , C22B7/003 , C22B11/025 , C22B15/0058 , C22B23/026 , Y02P10/214 , Y02P10/22 , Y02P10/224
摘要: Cermet material obtained from unused inert anodes, used inert anodes and cermet used in the production of inert anodes is beneficiated into a nonferrous metal concentrate composition from which metal values contained in the composition may be readily recovered by using a conventional smelting process. The invention also relates to the use of the composition in a smelting process for the recovery of metal values from the cermet composition of the invention.
摘要翻译: 从惰性阳极中使用的惰性阳极,使用惰性阳极和金属陶瓷得到的金属陶瓷材料被精选成有色金属浓缩组合物,组合物中所含的金属值可以通过常规熔炼方法容易地回收。 本发明还涉及组合物在冶炼方法中用于从本发明的金属陶瓷组合物中回收金属值的用途。
-
公开(公告)号:US20040177721A1
公开(公告)日:2004-09-16
申请号:US10387505
申请日:2003-03-14
IPC分类号: C22B001/248
CPC分类号: C22B1/2406 , C22B7/003 , C22B11/025 , C22B15/0058 , C22B23/026 , Y02P10/214 , Y02P10/22 , Y02P10/224
摘要: Cermet material obtained from unused inert anodes, used inert anodes and cermet used in the production of inert anodes is beneficiated into a nonferrous metal concentrate composition from which metal values contained in the composition may be readily recovered by using a conventional smelting process. The invention also relates to the use of the composition in a smelting process for the recovery of metal values from the cermet composition of the invention.
摘要翻译: 从惰性阳极中使用的惰性阳极,使用惰性阳极和金属陶瓷得到的金属陶瓷材料被精选成有色金属浓缩组合物,组合物中所含的金属值可以通过常规熔炼方法容易地回收。 本发明还涉及组合物在冶炼方法中用于从本发明的金属陶瓷组合物中回收金属值的用途。
-