公开(公告)号:US5580474A
公开(公告)日:1996-12-03
申请号:US458799
申请日:1995-06-02
申请人: Walt Smith
发明人: Walt Smith
CPC分类号: B23K9/287
摘要: The present invention is a receiver made by a welding process. The receiver made according to this process has less net distortion because of a number of techniques used in the process, including: (1) cooling the weld with Carbon Dioxide (CO.sub.2) preheated with the welding torch tip; (2) use of not more than approximately 4% oxygen in the shield gas to enable hotter, faster welding; (3) the use of a reduced voltage and wire feed rate at the end of a weld to avoid cracking; (4) the intentional use of distortion to reduce net distortion; and (5) sequencing of welds to reduce distortion. Distortion can be introduced in the stamped parts as they are made or when placed in a fixture for welding that, when welded, have less distortion than before. Distortion can also be countered by welding parts in a sequence where a subsequent weld reduces the distortion of a previous weld.
摘要翻译: 本发明是通过焊接工艺制造的接收器。 根据该方法制造的接收器由于在该过程中使用的许多技术而具有较少的净变形,包括:(1)用焊枪尖预热的二氧化碳(CO 2)冷却焊缝; (2)在保护气体中使用不超过约4%的氧气以实现更热,更快速的焊接; (3)焊缝末端采用降低电压和送丝速度,避免开裂; (4)有意使用失真减少网络失真; 和(5)焊缝排序以减少变形。 扭曲可以在冲压部件中进行,因为它们被制成或当被放置在用于焊接的夹具中时,当被焊接时,具有比以前更小的变形。 也可以通过焊接部件以后续焊接减少先前焊缝的变形的顺序来抵消变形。
-
公开(公告)号:US5440099A
公开(公告)日:1995-08-08
申请号:US172836
申请日:1993-12-22
申请人: Walt Smith
发明人: Walt Smith
CPC分类号: B23K9/287
摘要: The present invention is a method for welding difficult-to-weld metal components as illustrated in the welding of a receiver for a weapon. The method reduces net distortion by a number of techniques, including: (1) cooling the weld with Carbon Dioxide (CO.sub.2) preheated with the welding torch tip; (2) use of not more than approximately 4% oxygen in the shield gas to enable hotter, faster welding; (3) the use of a reduced voltage and wire feed rate at the end of a weld to avoid cracking; (4) the intentional use of distortion to reduce net distortion; and (5) sequencing of welds to reduce distortion. Distortion can be introduced in the stamped parts as they are made or when placed in a fixture for welding that, when welded, have less distortion than before. Distortion can also be countered by welding parts in a sequence where a subsequent weld reduces the distortion of a previous weld. The process is illustrated as applied to a receiver for a weapon made by welding non-compatible and low carbon steels in a low tolerance configuration.