公开(公告)号:US20110045316A1
公开(公告)日:2011-02-24
申请号:US12917109
申请日:2010-11-01
申请人: Werner BRANDSTÄTTER , Herbert EIBENSTEINER , Martin FLEISCHANDERL , Josef FADERL , Gerald LANDL , Anna Elisabeth RAAB , Siegfried KOLNBERGER
发明人: Werner BRANDSTÄTTER , Herbert EIBENSTEINER , Martin FLEISCHANDERL , Josef FADERL , Gerald LANDL , Anna Elisabeth RAAB , Siegfried KOLNBERGER
CPC分类号: C21D1/673 , C21D9/46 , C21D2221/00 , C21D2251/02 , C25D5/36 , C25D5/48 , Y10T29/49982 , Y10T29/49995 , Y10T428/12799 , Y10T428/31678
摘要: The invention relates to a method for producing a hardened profiled structural part from a hardenable steel alloy with cathodic corrosion protection. The method includes applying a coating to a sheet made of a hardenable steel alloy, wherein the coating comprises zinc, and the coating further comprises one or several elements with affinity to oxygen in a total amount of 0.1 weight-% to 15 weight-% in relation to the total coating. After applying the coating, the coated sheet steel is roller-profiled in a profiling device, so that the sheet tape is formed into a roller-formed profiled strand. Thereafter, the coated sheet steel is brought, at least in parts and with the admission of atmospheric oxygen, to a temperature required for hardening and is heated to a structural change required for hardening. A skin made of an oxide of the element(s) with affinity to oxygen is formed on the surface of the coating. After sufficient heating the sheet is cooled, wherein the rate of cooling is set in such a way that hardening of the sheet alloy is achieved. The invention further relates to a corrosion-protection layer and a profiled structural element.
摘要翻译: 本发明涉及一种由具有阴极腐蚀保护性的可硬化钢合金制造硬化型材结构件的方法。 该方法包括将涂层施加到由可硬化钢合金制成的片材上,其中所述涂层包含锌,并且所述涂层还包含一种或几种与氧的亲和性的总量为0.1重量%至15重量%的元素 与总涂层的关系。 涂覆涂层后,将涂覆的钢板在成型装置中进行辊压成型,使得片材带形成为辊状成形的股线。 此后,将涂覆钢板至少部分地并且承受大气中的氧气带到硬化所需的温度,并被加热到硬化所需的结构变化。 在涂层的表面上形成由与氧相容的元素的氧化物制成的皮肤。 在充分加热之后,片材被冷却,其中冷却速率设定为使得实现了片状合金的硬化。 本发明还涉及一种防腐蚀层和异型结构元件。