公开(公告)号:US4793542A
公开(公告)日:1988-12-27
申请号:US138050
申请日:1987-12-28
申请人: Wolfgang Farrenkopf , Heinrich Gruenauer , Manfred Menzinger , Joachim von Hirsch , Reinhard Opitz
发明人: Wolfgang Farrenkopf , Heinrich Gruenauer , Manfred Menzinger , Joachim von Hirsch , Reinhard Opitz
IPC分类号: B23K20/12
CPC分类号: B23K20/129 , B23K2203/04 , B23K2203/06 , B23K2203/18
摘要: An improved friction-welding process for effecting a joint between steel and nodular graphite-containing cast iron by using (i) a short friction-generating time so as to minimize diffusion of carbon into steel and (ii) an elevated forging pressure so as to effect a quantitative ejection of carburized melt but avoid formation of a weld laminate, is provided, as well as a nodular graphite-containing cast iron of grade 40.3 S, suitable for use in friction-welding and comprising about 280-320 graphite nodules per mm.sup.2, 280-300 ferrite grains per mm.sup.2 and a spherulite proportion of about at least 95% by weight of the graphite precipitations.
摘要翻译: 一种改进的摩擦焊接方法,用于通过使用(i)短的摩擦产生时间来实现钢和含节结构的含石墨的铸铁之间的接合,以使碳的扩散最小化到钢中,和(ii)升高的锻造压力,以便 实现渗碳熔体的定量喷射,但避免形成焊接层压板,以及适用于摩擦焊接的含有40.3 S的球墨铸铁,其包含约280-320个石墨结核/ mm2 ,280-300铁素体颗粒/ mm 2,球晶比例约为石墨沉淀物重量的至少95%。