Copolymer and preparation method and application thereof
    1.
    发明授权
    Copolymer and preparation method and application thereof 有权
    共聚物及其制备方法及应用

    公开(公告)号:US08623791B2

    公开(公告)日:2014-01-07

    申请号:US13244102

    申请日:2011-09-23

    IPC分类号: C09K8/12 C09K8/32 C09K8/588

    CPC分类号: C08F230/04 C09K8/12

    摘要: A copolymer and preparation method and application thereof are disclosed. The copolymer is random copolymer obtained from monomers consisting of acrylamide, acrylic acid, alkenyl sulfonate, 2-acrylamido-dodecyl sulfonate, p-styrene sulfonate or isoprene sulfonate and so on. The copolymer of present invention can be used as fluid loss additive and has good fluid loss properties, which would not make the drilling fluid thicken at high temperature of 200° C. and high salt conditions of saturated brine. It has a medium-pressure fluid loss after aging and rolling for 16 h at high temperature of 200° C., as measured in accordance with the American Petroleum Institute Standard Test at room temperature, and has good properties of high temperature-resisting and salt-resisting.

    摘要翻译: 公开了共聚物及其制备方法和应用。 共聚物是由丙烯酰胺,丙烯酸,链烯基磺酸酯,2-丙烯酰氨基 - 十二烷基磺酸酯,对苯乙烯磺酸酯或异戊二烯磺酸酯等单体组成的无规共聚物。 本发明的共聚物可用作流体损失添加剂,具有良好的流体损失性能,不会使钻井液在200℃的高温和饱和盐水的高盐条件下变稠。 根据美国石油学会标准试验在室温下测量,在200℃的高温下老化和轧制16小时后,中压流体损失具有良好的耐高温和耐盐性能 保留。

    COPOLYMER AND PREPARATION METHOD AND APPLICATION THEREOF
    2.
    发明申请
    COPOLYMER AND PREPARATION METHOD AND APPLICATION THEREOF 有权
    共聚物及其制备方法及应用

    公开(公告)号:US20120077718A1

    公开(公告)日:2012-03-29

    申请号:US13244102

    申请日:2011-09-23

    IPC分类号: C09K8/12 C08F230/04

    CPC分类号: C08F230/04 C09K8/12

    摘要: A copolymer and preparation method and application thereof are disclosed. The copolymer is random copolymer obtained from monomers consisting of acrylamide, acrylic acid, alkenyl sulfonate, 2-acrylamido-dodecyl sulfonate, p-styrene sulfonate or isoprene sulfonate and so on. The copolymer of present invention can be used as fluid loss additive and has good fluid loss properties, which would not make the drilling fluid thicken at high temperature of 200° C. and high salt conditions of saturated brine. It has a medium-pressure fluid loss after aging and rolling for 16 h at high temperature of 200° C., as measured in accordance with the American Petroleum Institute Standard Test at room temperature, and has good properties of high temperature-resisting and salt-resisting.