公开(公告)号:US20120067470A1
公开(公告)日:2012-03-22
申请号:US13319600
申请日:2010-05-13
申请人: Yoshihiro Serizawa , Yasuhiro Nishiyama , Shigeru Ogawa , Shinji Ida , Hitoshi Nikaidoh , Isao Yoshii , Noriyuki Hishinuma , Tetsuo Kishimoto , Nobuhiro Takagi
发明人: Yoshihiro Serizawa , Yasuhiro Nishiyama , Shigeru Ogawa , Shinji Ida , Hitoshi Nikaidoh , Isao Yoshii , Noriyuki Hishinuma , Tetsuo Kishimoto , Nobuhiro Takagi
CPC分类号: B21B45/0218
摘要: The present invention provides a method of cooling a hot-rolled steel strip which has passed through a finishing rolling, including: cooling the hot-rolled steel strip from a first temperature of not lower than 600° C. and not higher than 650° C. to a second temperature of not higher than 450° C. with cooling water having the water amount density of not lower than 4 m3/m2/min and not higher than 10 m3/m2/min, wherein with respect to the area of the target surface, the area of a portion where a plurality of spray jets of the cooling water directly strikes on the target surface is at least 80%.
-
公开(公告)号:US08920708B2
公开(公告)日:2014-12-30
申请号:US13584973
申请日:2012-08-14
申请人: Yoshihiro Serizawa , Yasuhiro Nishiyama , Shigeru Ogawa , Shinji Ida , Hitoshi Nikaidoh , Isao Yoshii , Noriyuki Hishinuma , Tetsuo Kishimoto , Nobuhiro Takagi
发明人: Yoshihiro Serizawa , Yasuhiro Nishiyama , Shigeru Ogawa , Shinji Ida , Hitoshi Nikaidoh , Isao Yoshii , Noriyuki Hishinuma , Tetsuo Kishimoto , Nobuhiro Takagi
CPC分类号: B21B45/0218
摘要: The present invention provides a method of cooling a hot-rolled steel strip which has passed through a finishing rolling, including: cooling the hot-rolled steel strip from a first temperature of not lower than 600° C. and not higher than 650° C. to a second temperature of not higher than 450° C. with cooling water having the water amount density of not lower than 4 m3/m2/min and not higher than 10 m3/m2/min, wherein with respect to the area of the target surface, the area of a portion where a plurality of spray jets of the cooling water directly strikes on the target surface is at least 80%.
摘要翻译: 本发明提供一种通过精轧的冷轧钢带的冷却方法,其特征在于,包括:将所述热轧钢带从不低于600℃且不高于650℃的第一温度冷却 至不超过450℃的第二温度,其中水量密度不低于4m 3 / m 2 / min且不高于10m 3 / m 2 / min的冷却水,其中相对于 目标表面,冷却水的多个喷射射流直接撞击目标表面的部分的面积为至少80%。
-
公开(公告)号:US08414716B2
公开(公告)日:2013-04-09
申请号:US13319600
申请日:2010-05-13
申请人: Yoshihiro Serizawa , Yasuhiro Nishiyama , Shigeru Ogawa , Shinji Ida , Hitoshi Nikaidoh , Isao Yoshii , Noriyuki Hishinuma , Tetsuo Kishimoto , Nobuhiro Takagi
发明人: Yoshihiro Serizawa , Yasuhiro Nishiyama , Shigeru Ogawa , Shinji Ida , Hitoshi Nikaidoh , Isao Yoshii , Noriyuki Hishinuma , Tetsuo Kishimoto , Nobuhiro Takagi
IPC分类号: C21D8/02
CPC分类号: B21B45/0218
摘要: The present invention provides a method of cooling a hot-rolled steel strip which has passed through a finishing rolling, including: cooling the hot-rolled steel strip from a first temperature of not lower than 600° C. and not higher than 650° C. to a second temperature of not higher than 450° C. with cooling water having the water amount density of not lower than 4 m3/m2/min and not higher than 10 m3/m2/min, wherein with respect to the area of the target surface, the area of a portion where a plurality of spray jets of the cooling water directly strikes on the target surface is at least 80%.