公开(公告)号:US06608118B2
公开(公告)日:2003-08-19
申请号:US10083152
申请日:2002-02-27
申请人: Yukishiro Kosaka , Genjiro Hattori , Hidero Suzuki , Satoshi Kondo , Masahiro Fukuyama , Atsushi Ichinose
发明人: Yukishiro Kosaka , Genjiro Hattori , Hidero Suzuki , Satoshi Kondo , Masahiro Fukuyama , Atsushi Ichinose
IPC分类号: C08J900
CPC分类号: A47L17/08 , B29C44/5636
摘要: A melamine molded foam is produced by heat-compressing a melamine foam to a thickness of {fraction (1/1.2)} to {fraction (1/12)} to cause plastic deformation and temporarily fixing the shape; the heat-compression is performed under the conditions of from 210 to 350° C. for 3 minutes or longer; the heat-compression is preferably performed at a temperature within the range of lower than the decomposition temperature of the melamine monomer by 140° C. or less; in some of such molded foams, the shape recovery in the direction of thickness with the lapse of time is observed depending upon the heat-compression conditions; and the dimensional recovery ratio is 40% or less when allowed to stand at 23° C. for 200 hours.