POSITIVE ELECTRODE ACTIVE MATERIAL PRODUCTION METHOD, POSITIVE ELECTRODE, AND STORAGE DEVICE
    1.
    发明申请
    POSITIVE ELECTRODE ACTIVE MATERIAL PRODUCTION METHOD, POSITIVE ELECTRODE, AND STORAGE DEVICE 审中-公开
    正极电极活性材料生产方法,正电极和存储装置

    公开(公告)号:US20130071749A1

    公开(公告)日:2013-03-21

    申请号:US13613245

    申请日:2012-09-13

    IPC分类号: H01M4/58 H01M4/583

    摘要: There is provided a positive electrode active material production method, a positive electrode, and a storage device. A production method of a positive electrode active material having a LiVPO4F-type crystal structure and containing carbon, includes: a step of synthesizing a precursor that has VPO4 containing carbon, from a starting material in the form of vanadium pentoxide and a phosphate compound, and from a carbon material as an additive; and a step of synthesizing LiVPO4F containing carbon, from the precursor and LiF. The carbon material as an additive is conductive carbon black having a specific surface area of 700 to 1500 m2/g, and in the step of synthesizing the precursor, an addition amount of the conductive carbon black is less than 2 moles per mole of vanadium pentoxide.

    摘要翻译: 提供正极活性物质的制造方法,正极和存储装置。 具有LiVPO 4 F型结晶结构并含有碳的正极活性物质的制造方法包括:从五氧化二钒和磷酸盐化合物的原料合成含有含有VPO 4的前体的工序,以及 从碳材料作为添加剂; 以及从前体和LiF合成含有碳的LiVPO 4 F的工序。 作为添加剂的碳材料是比表面积为700〜1500m 2 / g的导电性炭黑,在合成前体的步骤中,每摩尔五氧化二钒的导电性炭黑的添加量少于2摩尔 。