Abstract:
The invention is: a fiber produced by forming a fiber using pellets, and annealing the fiber at 150 to 220° C., the pellets being formed of a resin powder of a cycloolefin polymer, the resin powder having a loose bulk density of 0.3 to 0.6 g/cc when measured using 100 cc of the resin powder: a method for producing the fiber. The invention provides a method for producing a cycloolefin polymer fiber that exhibits good productivity and strength during spinning, and a low thermal shrinkage ratio.
Abstract:
A resin composition including a resin component and glass fibers, the resin component including 0 to 99 wt % of a hydrogenated crystalline cycloolefin ring-opening polymer that includes a repeating unit derived from a polycyclic norbornene-based monomer that includes 3 or more rings, and does not include a polar group, and 1 to 100 wt % of a hydrogenated modified crystalline cycloolefin ring-opening polymer that includes a repeating unit derived from a polycyclic norbornene-based monomer that includes 3 or more rings, and includes a polar group, the resin composition including the glass fibers in an amount of 5 to 150 parts by weight based on 100 parts by weight of the resin component; and a resin formed article obtained by forming the resin composition.