公开(公告)号:US20120088868A1
公开(公告)日:2012-04-12
申请号:US13377911
申请日:2010-07-01
申请人: Anteneh Z. Worku , Kim L. Walton , Henry G. Heck
发明人: Anteneh Z. Worku , Kim L. Walton , Henry G. Heck
IPC分类号: C08K5/3477 , C08K5/52 , C08K5/3492 , C08K5/5397
CPC分类号: C08L23/12 , C08K3/34 , C08K5/34928 , C08K5/49 , C08L23/0815 , C08L2201/02 , C08L2666/06
摘要: The invention provides a polyolefin composition comprising: A) a propylene-based polymer having a flex modulus of greater than 1500 MPa and an HDT of greater than 100° C.; B) an ethylene/α-olefin interpolymer having Tg of less than −30° C., a tan delta, measured at 0.1 radians/s at 190° C., of less than 3, an HDT that is greater than, or equal to, the peak melting temperature of the ethylene/α-olefin interpolymer, measured by differential scanning calorimetry; and C) a fiber filler; and D) a nitrogen source and/or a phosphorus source, wherein at least one source is derived from at least one organic compound, or salt thereof; and wherein the weight ratio of the propylene-based polmer:ethylene/α-olefin interpolymer (A:B) is from 9:1 to 6:4.
摘要翻译: 本发明提供一种聚烯烃组合物,其包含:A)弹性模量大于1500MPa,HDT大于100℃的丙烯类聚合物; B)Tg小于-30℃的乙烯/α-烯烃互聚物,在190℃下以0.1弧度/秒测量的tanδ小于3的HDT,大于或等于 通过差示扫描量热法测定乙烯/α-烯烃互聚物的峰值熔融温度; 和C)纤维填料; 和D)氮源和/或磷源,其中至少一种源衍生自至少一种有机化合物或其盐; 丙烯类聚合物:乙烯/α-烯烃互聚物(A:B)的重量比为9:1〜6:4。