公开(公告)号:US4747890A
公开(公告)日:1988-05-31
申请号:US911067
申请日:1986-09-24
申请人: Philippe Meyer
发明人: Philippe Meyer
CPC分类号: C22C21/10 , F17C1/14 , F17C2201/0104 , F17C2201/058 , F17C2203/0646 , F17C2203/0648 , F17C2209/21 , F17C2260/011 , F17C2260/017
摘要: The invention relates to hollow bodies for gas under pressure manufactured from an aluminum alloy containing Zn, Cu and Mg as principal alloying elements and intended in particular for the production of metal bottles for pressurized gas. The hollow bodies are manufactured from an alloy consisting essentially of (in % by weight):______________________________________ 6.25 .ltoreq. Zn .ltoreq. 8.0 Mn .ltoreq. 0.20 1.2 .ltoreq. Mg .ltoreq. 1.95 Zr .ltoreq. 0.05 1.7 .ltoreq. Cu .ltoreq. 2.8 Ti .ltoreq. 0.05 0.15 .ltoreq. Cr .ltoreq. 0.28 Others each .ltoreq.0.05 Fe .ltoreq. 0.20 Others total .ltoreq.0.15 Si + Fe .ltoreq. 0.40 Balance Al. ______________________________________ The alloy in state T73 complies with the very severe technical requirements in respect of strength and ductility which are imposed in relation to use for hollow bodies under pressure.
摘要翻译: 本发明涉及由含有Zn,Cu和Mg作为主要合金元素的铝合金制成的压力气体中空体,特别用于生产用于加压气体的金属瓶。 中空体由基本上由(以重量%计)合金组成的合金制成:-6.25≤Zn≤8.0Mn≤0.20-2.2Mg / = 1.95 Zr = 0.05-1.7 = Cu = 2.8 Ti = 0.05 -0.15 = Cr = 0.28其他各自 = 0.05 -Fe <0.20其他总数<= 0.15 -Si + Fe <= 0.40平衡 Al。 - 状态T73中的合金符合强度和延展性的非常严格的技术要求,这些技术要求与在压力下的中空体的使用有关。