NECK RING AND METHOD OF MAKING FOR A GLASS CONTAINER FORMING MACHINE
    1.
    发明申请
    NECK RING AND METHOD OF MAKING FOR A GLASS CONTAINER FORMING MACHINE 审中-公开
    玻璃容器成型机的NECK环和方法

    公开(公告)号:WO2010051060A2

    公开(公告)日:2010-05-06

    申请号:PCT/US2009/039845

    申请日:2009-04-08

    CPC classification number: C03B9/325 C03B9/48 Y02P40/57

    Abstract: A neck ring for molding a glass container neck finish that includes at least one closure attachment feature. The neck ring includes two semi-annular bi-metal neck ring sections (12, 14), each consisting essentially of a neck ring insert (20, 22) of wear- resistant metal construction and a neck ring body (16, 18) of heat-conductive metal construction different from said wear-resistant metal construction and formed around said neck ring insert so as to embed it in said neck ring body. Each of said neck ring halves has a glass-contacting cavity face that includes a first surface portion (30, 32) formed by said inserts for molding the at least one closure attachment feature on the neck finish and a second surface portion (34, 36) formed by said bodies for molding portions of the neck finish excluding the at least one closure attachment feature.

    Abstract translation: 用于模制玻璃容器颈部的颈环,其包括至少一个闭合附接特征。 颈环包括两个半环形双金属颈环部分(12,14),每个部分基本上由耐磨金属结构的颈环插入件(20,22)和颈环本体(16,18)组成, 导热金属结构与所述耐磨金属结构不同,并形成在所述颈环插入件周围,以便将其嵌入所述颈环体中。 每个所述颈环半部具有玻璃接触腔体面,其包括由所述插入件形成的第一表面部分(30,32),用于模制颈部末端上的至少一个封闭件附接特征;以及第二表面部分(34,36 )由所述主体形成,用于模制除了所述至少一个闭合附接特征之外的所述颈部完成部分。

    A METHOD OF EXTENDING THE LIFESPAN OF A METAL CAVITY MOULD
    2.
    发明申请
    A METHOD OF EXTENDING THE LIFESPAN OF A METAL CAVITY MOULD 审中-公开
    扩展金属腔模具寿命的方法

    公开(公告)号:WO2009090622A1

    公开(公告)日:2009-07-23

    申请号:PCT/IB2009/050178

    申请日:2009-01-19

    Abstract: A method of extending the lifespan of a metal cavity glass bottle mould, includes the steps of machining the entire moulding surface of the mould to remove a surface layer of metal, cladding the machined moulding surface by depositing a layer of filler metal onto the surface in a laser cladding process and machining an exposed surface of the cladding layer so as to remove excess filler metal and return the moulding cavity to its design dimensions. The method includes a method of repairing a metal cavity mould by removing surface defects in the moulding surface of a damaged mould by machining the moulding surface and thereafter cladding the moulding surface. The method extends to the cladding of the moulding surface of an undamaged metal cavity mould.

    Abstract translation: 一种延长金属腔玻璃瓶模具使用寿命的方法包括以下步骤:加工模具的整个模制表面以去除金属表面层,通过在表面上沉积一层填充金属来包覆机加工的模制表面 激光熔覆工艺并加工包覆层的暴露表面,以便去除多余的填充金属并将模制腔返回到其设计尺寸。 该方法包括通过机械加工模制表面并且然后包覆模制表面来去除损坏的模具的模制表面中的表面缺陷来修复金属腔模具的方法。 该方法延伸到未损坏的金属腔模具的模制表面的包层。

    METHOD FOR MANUFACTURING A HOLLOW GLASS PUNCH FOR PIECE MOLDING
    5.
    发明申请
    METHOD FOR MANUFACTURING A HOLLOW GLASS PUNCH FOR PIECE MOLDING 审中-公开
    一种中空玻璃打孔机的制造方法

    公开(公告)号:WO1981001841A1

    公开(公告)日:1981-07-09

    申请号:PCT/CH1980000160

    申请日:1980-12-22

    Inventor: CASTOLIN SA

    CPC classification number: C03B9/48 B22D23/003 C23C4/185

    Abstract: A compact layer (3) of material is formed by thermal projection on a support piece (1) of which at least the surface portion is made of a material having the property of preventing adhesion of this layer (3) on said support (1) and on the adjacent portion (4) of a piece (2) acting as a base for the punch and the support piece (1) is separated from the projected layer (3) by maintaining the integrity, on the one hand of the assembly formed by the projected layer (3) and the piece (2) acting as a base for the punch, and on the other hand, of the support piece (1). The punch thus obtained is comprised of a hollow body with thin walls having a high mechanical strength.

    Abstract translation: 材料的致密层(3)通过在支撑件(1)上的热投影形成,其至少表面部分由具有防止该层(3)粘附在所述支撑件(1)上的特性的材料制成, 并且在作为冲头的基座的件(2)的相邻部分(4)上,并且支撑件(1)通过保持完整性与突出层(3)分离,一方面形成 通过投影层(3)和用作冲头的基座的片(2),另一方面,作为支撑件(1)。 由此获得的冲头由具有高机械强度的薄壁的中空体构成。

    ガラス成形金型、その製造方法、及びガラス成形体の製造方法。
    6.
    发明申请
    ガラス成形金型、その製造方法、及びガラス成形体の製造方法。 审中-公开
    用于模制玻璃的模具,其生产方法和生产玻璃模制产品的方法

    公开(公告)号:WO2010143320A1

    公开(公告)日:2010-12-16

    申请号:PCT/JP2009/067556

    申请日:2009-10-08

    CPC classification number: C03B9/48 C03B11/086

    Abstract:  成形時における成形金型の成形面の温度を上げることなく、胴部の膨らみ、合目線の顕著化の欠点の発生を防止し、エネルギーを節約する。また、梨地模様などの凹凸模様がガラス成形品表面に明確に表れるようにする。 金型の形成面の熱放射率を0.85以上にすることで、前記課題が解決される。熱放射率を0.85以上とするためには、成形面に熱放射率が高い物質の被膜を形成する。この被膜としては、黒錆び、黒クロム等のめっきやPVD処理、黒体塗料等がある。黒錆は、成形面に酸溶液を塗布した後、加熱処理を行うことで容易に形成できる。

    Abstract translation: 用于成型玻璃的模具,其防止在模制中不发生诸如体部的凸起或接缝线的独特性的缺陷,而不增加模具的模制表面温度,并且其降低能量消耗并且可以应用 在玻璃模制产品的表面上具有诸如点状设计的清晰的压花设计。 该模具具有0.85或更高的热辐射率的模塑表面。 0.85以上的发热率可以通过在成形面上形成具有高热辐射率的物质的涂层来实现。 涂层是黑锈,黑色镀铬,通过PVD处理形成的黑色铬沉积物,黑色涂层等。 通过将酸溶液施加到成型面上并对所得到的成形面进行热处理,可以容易地形成黑锈。

    A COATED MOULD AND PROCESS FOR PRODUCING THE MOULD
    8.
    发明申请
    A COATED MOULD AND PROCESS FOR PRODUCING THE MOULD 审中-公开
    用于生产模具的涂层模具和工艺

    公开(公告)号:WO01028942A1

    公开(公告)日:2001-04-26

    申请号:PCT/EP2000/010368

    申请日:2000-10-20

    CPC classification number: C03B40/00 C03B9/48 C23C4/00 C23C4/08

    Abstract: An improved mould (10) for use in the production of glass containers such as bottles, jars and the like, the mould (10) includes at least one mould surface defining a cavity (14) which is adapted to receive molten glass, and in which the mould (10) surface is provided with a coating (16) over substantially the whole of the surface, the coating comprising an alloy. The mould (10) is made of segments or partial sections - preferably of two half bodies (12 12a) - with a hollow space (14) in each segment or half body (12, 12a). In the hollow space (14) the coating (16) - comprising an alloy of cobalt and nickel - is metallurgically bonded to the mould (10). The process for producing the mould (10) includes that the coating (16) is fused to the mould (10) by using a two-stage process in which a powder containing the constituent elements of the alloy coating (16) is initially provided, the powder comprises a specially formulated alloy powder in which each particle essentially comprises the elements of the final alloy coating (16) or the coating (16) comprises one or more different powders which maybe mixed together.

    Abstract translation: 一种用于生产诸如瓶子,瓶子等玻璃容器的改进的模具(10),所述模具(10)包括限定适于接收熔融玻璃的空腔(14)的至少一个模具表面,并且 其中模具(10)表面在基本上整个表面上设置有涂层(16),所述涂层包括合金。 模具(10)由每个段或半体(12,12a)中的中空空间(14)的段或部分部分 - 优选地由两个半体(12 12a)构成。 在中空空间(14)中,包含钴和镍的合金的涂层(16)被冶金地结合到模具(10)上。 用于制造模具(10)的方法包括通过使用其中最初设置含有合金涂层(16)的构成元素的粉末的两阶段工艺将涂层(16)熔合到模具(10) 粉末包括特殊配制的合金粉末,其中每个颗粒基本上包括最终合金涂层(16)的元件,或者涂层(16)包含可混合在一起的一种或多种不同的粉末。

    COATED PART, COATING AND METHOD OF COATING
    9.
    发明申请
    COATED PART, COATING AND METHOD OF COATING 审中-公开
    涂层,涂料和涂料方法

    公开(公告)号:WO98057804A1

    公开(公告)日:1998-12-23

    申请号:PCT/US1998/011286

    申请日:1998-05-29

    Abstract: A corrosion and erosion resistant article having good release characteristics which includes a metal body having a first surface thereon and a base coat adhered to the first surface has been invented. The base coat comprises at least one layer of inorganic particulate material bonded to the first surface. A second coat adheres to the base coat. The second coat comprises a cured coating of solid particulate lubricant in a phosphate/chromate metal ion solution. A method of applying a corrosion and erosion resistant coating having good release characteristics had been invented. The method comprises providing a metal body having a first surface thereon and applying a base coat to the first surface where the base coat comprises at least one layer of inorganic particulate material bonded to the first surface. The next step comprises partially curing the base coat and applying a second coat that adheres to the base coat, the second coat comprises a cured coating of solid particulate lubricant in a phosphate/chromate metal ion solution. A third coat may be applied.

    Abstract translation: 已经发明了具有良好剥离特性的抗腐蚀和耐腐蚀制品,其包括其上具有第一表面的金属体和粘附到第一表面的底涂层。 底涂层包含至少一层结合到第一表面的无机颗粒材料。 第二层涂层粘附到底漆上。 第二层包括在磷酸盐/铬酸盐金属离子溶液中的固体颗粒润滑剂的固化涂层。 已经发明了一种施加具有良好剥离特性的耐腐蚀和耐腐蚀涂层的方法。 该方法包括在其上提供具有第一表面的金属体,并将基底涂层施加到第一表面,其中基底涂层包含至少一层结合到第一表面的无机颗粒材料。 下一步骤包括部分固化底涂层并施加附着于底涂层的第二涂层,第二涂层包含在磷酸盐/铬酸盐金属离子溶液中的固体颗粒润滑剂的固化涂层。 可以应用第三层。

    GLASSWORKS MOLDS AND UTILIZATION THEREOF
    10.
    发明申请
    GLASSWORKS MOLDS AND UTILIZATION THEREOF 审中-公开
    玻璃工具的使用和使用

    公开(公告)号:WO1988004283A1

    公开(公告)日:1988-06-16

    申请号:PCT/FR1987000492

    申请日:1987-12-10

    CPC classification number: C03B9/48

    Abstract: Cast-iron mold for the production of glass containers by using a ''pressed-blown'' or ''blown-blown'' technique wherein the parts exposed to the parison are coated with a uniform alumina layer of which the thickness is less than 5 micrometers. The invention applies to industrial techniques for producing glass containers such as bottles, flasks, jars or the like.

    Abstract translation: 通过使用“吹吹”或“吹塑”技术生产玻璃容器的铸铁模具,其中暴露于型坯的部件涂覆有均匀的氧化铝层,其厚度小于 5微米。 本发明适用于制造瓶,瓶,罐等玻璃容器的工业技术。