1.
公开(公告)号:WO2011127873A2
公开(公告)日:2011-10-20
申请号:PCT/CZ2011/000034
申请日:2011-04-12
Applicant: ŠKUTCHANOVÁ, Zuzana
Inventor: ŠKUTCHANOVÁ, Zuzana
CPC classification number: A45D29/04 , C03C17/3411 , C03C2217/42 , C03C2217/77
Abstract: Manufacturing method of grinding surface on glass cosmetics, in particular the nail and skin file, from flat glass of FLOAT type, is carried out by marking at least one abrasive surface on one or two sides of a glass pane or intermediate product. This surface is then coated with fusing glue, powdered with clean quartz sand with grain size between 1 and 500 μm using a sieve, and the surplus sand is knocked-down. The intermediate product with fixed sand is inserted into the fusing furnace where it is baked at the temperature of up to 900°C. The abrasive surface may be roughened by sand blasting before the fusing glue application; the intermediate product coated with fusing glue can be decorated with glass fritte.
Abstract translation: 通过在玻璃板或中间产品的一侧或两侧标记至少一个研磨表面,进行FLOAT型平板玻璃上玻璃化妆品,特别是指甲和皮肤文件研磨表面的制造方法。 该表面用熔融胶涂上,用筛子粉碎成粒度为1〜500μm的干净的石英砂,多余的沙子被倒下。 将具有固定砂的中间产品插入定影炉中,其中在高达900℃的温度下烘烤。 在熔融粘合剂施加之前,研磨表面可以通过喷砂粗糙化; 涂有熔融胶的中间产品可以用玻璃料装饰。