含フッ素化合物の製造方法
    1.
    发明申请
    含フッ素化合物の製造方法 审中-公开
    生产氟化合物的方法

    公开(公告)号:WO2002060853A1

    公开(公告)日:2002-08-08

    申请号:PCT/JP2002/000795

    申请日:2002-01-31

    IPC分类号: C07C67/307

    摘要: A method of synthesizing in a high yield the target fluorine compound having a geminal-difluoro structure by subjecting an easily available carbonyl compound to a two-stage reaction. A compound (1) such as ethyl 4-oxocyclohexanecarboxylate is reacted with either a compound represented by the formula X-Z, such as phosphorus pentachloride, or a compound represented by the formula Z2O (wherein Z is a monovalent group which gives a leaving group of the structure -OZ; and X is chlorine, bromine, or iodine). Subsequently, a fluorinating agent which generates a fluorine anion, such as HF, is caused to act on the reaction product to obtain a fluorine compound (2) such as ethyl 4,4-difluorocyclohexanecarboxylate.

    摘要翻译: 通过使容易获得的羰基化合物进行两步反应,高产率地合成具有偕二氟结构的目标氟化合物的方法。 将化合物(1)如4-氧代环己烷羧酸乙酯与式XZ表示的化合物如五氯化磷或由式Z 2 O表示的化合物(其中Z是给出离去基团的一价基团 结构-OZ; X是氯,溴或碘)。 随后,使产生氟阴离子的氟化物如HF用作反应产物,得到4,4-二氟环己烷羧酸乙酯等氟化合物(2)。

    低反射ガラスおよびディスプレイ用保護板
    2.
    发明申请
    低反射ガラスおよびディスプレイ用保護板 审中-公开
    低反射玻璃和保护板用于显示

    公开(公告)号:WO2009131206A1

    公开(公告)日:2009-10-29

    申请号:PCT/JP2009/058134

    申请日:2009-04-24

    IPC分类号: G02B1/11 C03C17/34 G09F9/00

    摘要:  耐擦傷性、耐候性、生産性、および外観に優れる低反射ガラスおよびディスプレイ用保護板を提供する。  ガラス基板12と、ガラス基板12の表面に形成された反射防止膜14とを有し、反射防止膜14が、ガラス基板12側から順に中間層16と最外層18とを有し、最外層18が、Si原子、C原子よびO原子を含む層であり、かつSi原子、C原子およびO原子の合計100モル%のうちのC原子の含有量が、0.5~3モル%であり、中間層16が、(a)層(高屈折率層)または(b)層(光吸収層)である低反射ガラス10;および低反射ガラス10からなる支持基体と、該支持基体の反射防止膜が形成されていない面側に設けられた導電膜とを有するディスプレイ用保護板。

    摘要翻译: 公开了具有优异的耐刮擦性,耐候性,生产率和外观的低反射玻璃。 还公开了一种用于显示器的保护板。 具体公开了一种低反射玻璃(10),其包括形成在玻璃基板(12)的表面上的玻璃基板(12)和抗反射膜(14)。 防反射膜(14)包括从玻璃基板(12)侧依次布置的中​​间层(16)和最外层(18),最外层(18)含有Si原子,C原子和O原子。 相对于Si原子,C原子和O原子的总共100摩尔%的C原子含量为0.5-3摩尔%。 中间层(16)由层(a)(高折射率层)或层(b)(光吸收层)构成。 用于显示器的保护板包括由低反射玻璃(10)构成的支撑体和形成在不形成防反射膜的支撑体侧的导电膜。