公开(公告)号:WO2011134025A1
公开(公告)日:2011-11-03
申请号:PCT/AU2011/000503
申请日:2011-04-29
Applicant: BORAL CEMENT LIMITED , LLOYD, Redmond Richard , KEYTE, Louise Margaret
Inventor: LLOYD, Redmond Richard , KEYTE, Louise Margaret
CPC classification number: C04B28/082 , C04B7/153 , C04B7/19 , C04B2111/00017 , C04B2111/00215 , Y02P40/143 , Y02W30/94 , C04B7/02 , C04B18/141 , C04B22/143 , C04B22/147 , C04B40/0608
Abstract: A unreacted dry cement composition or a cement composition comprising greater than 20wt% and less than 65wt% portland cement or clinker, granulated blast furnace slag optionally in combination with steel slag wherein the ratio of slag to cement or clinker is in the range of 1 :2 to 4:1, 1.5 - 6 wt% activator consisting of a sulphate of an alkali metal selected from the group of sodium (Na) and potassium (K) and optionally up to 10 wt% gypsum. A concrete composition comprising the cement composition, aggregate, water, and optional chemical admixtures is also claimed.
Abstract translation: 包含大于20重量%且小于65重量%的波特兰水泥或熟料,任选与钢渣组合的颗粒状高炉矿渣的未反应干燥水泥组合物或水泥组合物,其中渣与水泥或熟料的比例在1: 2至4:1,1.5-6重量%的活化剂,其由选自钠(Na)和钾(K)的组的碱金属的硫酸盐和任选的至多10重量%的石膏组成。 还要求包含水泥组合物,骨料,水和任选的化学混合物的混凝土组合物。